hottub.patents
Assignee / Organization

Friedmann James B.

7Total Forward Citations
3Indexed Patents
2Avg Citations / Patent
2Portfolio H-Index
US 2004062867 A1#23454813 Most Cited · 4 citations0.2/yr · PR 1.67PendingUS · Application
Method to reduce photoresist poisoning

A silicon rich anti-reflective coating ( 30 ) is formed on a layer ( 10 ) in which narrow linewidth features are to be formed. Prior to the formation of a photoresist layer ( 50 ), the anti-reflecting coating ( 30 ) is exposed to excited oxygen species to reduce photoresist…

US 2004253812 A1#29094490 Most Cited · 3 citations0.1/yr · PR 1.36PendingUS · Application
Method for BARC over-etch time adjust with real-time process feedback

A method for determining the anti-reflective coating (or bottom anti-reflective coating) over-etch time adjust with real-time process feedback is presented. The critical dimension CD resist of the patterned photoresist is measured and a first wafer with median values chosen (…

US 2005245088 A1#72441791 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Method for barc over-etch time adjust with real-time process feedback

A method for determining the anti-reflective coating (or bottom anti-reflective coating) over-etch time adjust with real-time process feedback is presented. The critical dimension CD resist of the patterned photoresist is measured and a first wafer with median values chosen (…