An elastomeric composition, and method of making the same, useful for forming thin films and sheets, comprising 55-60% hydrogenated SEEPS having a number average molecular weight of 90,000 to 100,000, 7-12% polystyrene, 15-30% oil, and 5 to 20% of an aliphatic hydrogenated…
Assignee / Organization
Foster Heith A
12Total Forward Citations
3Indexed Patents
4Avg Citations / Patent
2Portfolio H-Index
Key Inventors: Chapman Brian K Foster Heith A
An elastomeric composition, and method of making the same, useful for forming thin films and sheets, comprising 55-60% hydrogenated SEEPS having a number average molecular weight of 90,000 to 100,000, 7-12% polystyrene, 15-30% oil, and 5 to 20% of an aliphatic hydrogenated…