The present invention relates to a method for repairing or renewing cooling holes of a coated component of a gas turbine, having the following steps: - removal of an old coating from an outer side (2) of the component (1). The cooling hole (5) has an old cross section after…
Fernihough John
Process of masking cooling holes (4) of a gas turbine component (1) with an external surface (6), comprising a cavity (2) and a plurality of cooling holes (4) before coating the gas turbine component (1), comprising the steps of first applying a mask material (5) to the cooling…
Process of masking cooling holes (4) of a gas turbine component (1) with an external surface (6), comprising a cavity (2) and a plurality of cooling holes (4) before coating the gas turbine component (1), comprising the steps of first applying a mask material (5) to the cooling…
A method is disclosed of repairing cracks (5) on a surface (6) of a component (1) such as gas turbine components. The method comprises the steps of repairing the cracks (5) of the component by brazing, detecting by any means remaining cracks (5) on the surface (6) or below the…
A method is disclosed for recovering the properties of single crystal and directionally solidified Nickel based superalloys and articles made thereof, after use in a high temperature environment. The method comprises the steps of a stress relief treatment, a Ϝ' rejuvenation…
A method is disclosed for removing casting defects (5) from an article (1) with an oriented microstructure. The method comprises the steps of locating at least one casting defect (5) and melting the casting defect (5) locally by a heat source (7) to a depth at least as great as…
A method is disclosed for removing casting defects (5) from an article (1) with an oriented microstructure. The method comprises the steps of locating at least one casting defect (5) and melting the casting defect (5) locally by a heat source (7) to a depth at least as great as…