The invention relates to a glass ceramic, whereby the starting glass contains 35-65 wt. % Si02; 5-30 wt. % Na20; 0-20 wt. % K20; 5-30 wt. % Ca0; 0-10 wt. % Mg0; 0-5 wt. % Al203; 2-10 wt. % P205; 0-5 wt. % B203; 0.1-10 wt. % TiO2. The invention is characterised in that the…
Assignee / Organization
Fechner Joerg H
33Total Forward Citations
3Indexed Patents
11Avg Citations / Patent
3Portfolio H-Index
The alumino-silicate glass for lamp bulbs with molybdenum components contains alkaline earth metals and has the following composition (in % by weight based on oxide): SiO 2 >58 to 62, Al 2 O 3 15 to 17.5, MgO 0.1 to <1, CaO 5.5 to 14, SrO 0 to 8, BaO 6 to 17, ZrO 2 0 to 1,…
The invention relates to an alumino-silicate glass which has a thermal expansion coefficient in the range of 8 to 10×10 −6 /K in a temperature range of 20 to 300° C., a transformation temperature Tg in a range of 580° C. to 640° C., and a processing temperature VA in a range of…