A cycloolefin copolymer resin having a Hunter b color value of less than 1.0, which resin comprises: (a) a first cycloolefin copolymer having a glass transition temperature of from about 100° C. to about 220° C. and an intrinsic viscosity of from about 5 to about 1000 ml/g as…
Assignee / Organization
Dirk Heukelbach
8Total Forward Citations
2Indexed Patents
4Avg Citations / Patent
1Portfolio H-Index
The present invention relates to a process for reducing the toughness of moldings made from plastic, which comprises melting and mixing at least one semicrystalline polymer and at least one amorphous polyolefin in a heatable mixing assembly, processing the resultant mixture to…