Industrial materials can be efficiently pan granulated by grinding the material to 95% minus 150 mesh, feeding this to a pan in conjunction with 1 to 15% seed materials and applying binder solution such that the free moisture content of the green ball is between 8-13% by weight…
Derdall; Gary
Industrial materials can be efficiently pan granulated by grinding the material to 95% minus 150 mesh, feeding this to a pan in conjunction with 1 to 15% seed materials and applying binder solution such that the free moisture content of the green ball is between 8-13% by weight…
ABSTRACT OF THE DISCLOSURE A novel process for recovering hydrocarbon from a hydrocarbon bearing formation is disclosed. The process comprises introducing into the hydrocarbon bearing formation a hydrocarbon viscosity reducing agent selected from an aldehyde, an aldehyde forming…
ABSTRACT OF THE DISCLOSURE A process is disclosed for producing high brightness kaolin from ore containing silica, other types of clays, minerals such as ilmenite micas, feldspars and various metal silicates as well as organic matter. The process consists of sizing, a double…
A process is disclosed whereby an anion or base ion exchange resin in the hydroxy form is used to absorb sulphuric acid produced in the electrolysis of an alkali metal such as sodium sulphate and thereby enable production of an alkali metal hydroxide, e.g., caustic soda, without…
Industrial materials can be efficiently pan granulated by grinding the material to 95% minus 150 mesh, feeding this to a pan in conjunction with 1 to 15% seed materials and applying binder solution such that the free moisture content of the green ball is between 8-13% by weight…