A high-ductility high-carbon steel wire which is less apt to break during drawing and is used for steel cords, etc. It is a high-carbon steel wire produced by hot rolling and having a carbon content of 0.7% or higher. It comprises 95% or more pearlite structure, and the pearlite…
Demachi Hitoshi
A high-carbon steel wire rod of high ductility for steel cord and the like is provided that experiences little breakage during drawing. The high-carbon steel wire rod of high ductility is a high-carbon steel wire rod fabricated by hot rolling that that has a carbon content of…
Disclosed is a steel wire for a high strength spring. The wire is characterised by including, by mass%, at least 0.67% but less than 0.75% of C, 2.0-2.5% of Si, 0.5-1.2% of Mn, 0.8-1.3% of Cr, 0.03-0.20% of V, 0.05-0.25% of Mo, 0.05-0.30% of W and 0.003-0.007% of N, where the…
Deformed wire for a submarine optical fiber cable used for the pressure-proof layer of the submarine optical cable and having a high strength, that is, having a tensile strength of 1800 MPa or more, is provided, which deformed wire for reinforcing submarine optical fiber cable…
A high-carbon steel wire rod of high ductility for steel cord and the like is provided that experiences little breakage during drawing. The high-carbon steel wire rod of high ductility is a high-carbon steel wire rod fabricated by hot rolling that that has a carbon content of…
Provided is a wire rod contains, in mass %: C: 0.6 to 1.1%; Si: 0.1 to 0.5%; Mn: 0.2 to 0.6% ; S: 0.004 to 0.015%; and, Cr: 0.02 to less than 0.05%; with a balance including Fe and inevitable impurities in which P is limited to 0.02% by mass or lower and Al is limited to 0.003%…
High strength steel wire for spring containing, by mass %, C: 0.67% to less than 0.75%, Si: 2.0 to 2.5%, Mn: 0.5 to 1.2%, Cr: 0.8 to 1.3%, V: 0.03 to 0.20%, Mo: 0.05 to 0.25%, W: 0.05 to 0.30%, and N: 0.003 to 0.007%, having a total of contents of Mn and V of 0.70%≦Mn+V≦1.27%…
Provided is a wire material which contains 0.6-1.1 mass% C, 0.1-0.5 mass% Si, 0.2-0.6 mass% Mn, 0.004-0.015 mass% S, and 0.02-0.05 mass%, excluding 0.05 mass%, Cr, the remainder comprising Fe and incidental impurities in which the P and Al contents have been reduced to 0.02…
Provided is a wire rod contains, in mass %: C: 0.6 to 1.1%; Si: 0.1 to 0.5%; Mn: 0.2 to 0.6%; S: 0.004 to 0.015%; and, Cr: 0.02 to less than 0.05%; with a balance including Fe and inevitable impurities in which P is limited to 0.02% by mass or lower and Al is limited to 0.003%…
High strength steel wire for spring containing, by mass %, C: 0.67% to less than 0.75%, Si: 2.0 to 2.5%, Mn: 0.5 to 1.2%, Cr: 0.8 to 1.3%, V: 0.03 to 0.20%, Mo: 0.05 to 0.25%, W: 0.05 to 0.30%, and N: 0.003 to 0.007%, having a total of contents of Mn and V of 0.70%≦Mn+V≦1.27%…
A deformed wire for reinforcing a marine optical fiber cable used for the pressure-proof layer of the marine optical fiber cable and having a high strength of 1800 MPa or higher in tensile strength, characterized in that, by mass %, the requirement of 0.80 ≤ Ceq ≤ 1.80% is…