WO 2008/091520 A1#13654342 Most Cited · 8 citations0.4/yr · PR 1.68PendingWO · Application
Radiation cured elastomeric urethane acrylate films and the process for making same

A radiation-cured, elastomeric, urethane acrylate polymer has an elongation at break of between 100% (50) and 400% and a film break strength of between 200 and 2,600 psi at a thickness between about 0.002 inches and 0.010 inches.

US 2008176972 A1#19938529 Most Cited · 5 citations0.3/yr · PR 1.74PendingUS · Application
Radiation cured elastomeric urethane acrylate films and the process for making same

A radiation-cured, elastomeric, urethane acrylate polymer has an elongation at break of between 100% (50) and 400% and a film break strength of between 200 and 2,600 psi at a thickness between about 0.002 inches and 0.010 inches.

WO 2008/091520 A8#123332417 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Radiation cured elastomeric urethane acrylate films and the process for making same

A radiation-cured, elastomeric, urethane acrylate polymer has an elongation at break of between 100% (50) and 400% and a film break strength of between 200 and 2,600 psi at a thickness between about 0.002 inches and 0.010 inches.