Embodiments of the invention include a method for making optical fiber having reduced aging or hydrogen aging loss over the life of the fiber and optical fiber systems including such optical fibers. Improved silicon-oxygen stoichiometry during one or more preform manufacturing…
David Kalish
An expeditious method for introducing geometric perturbations into lightguide during fabrication offers a perturbation stream of amplitude and periodicity—constant or varying—to satisfy a variety of needs.
Embodiments of the invention include a method for making optical fibers that have reduced aging loss, hydrogen aging and other losses over the life of the fiber, and optical systems including such optical fibers. Improved conditions in fiber manufacturing environments are…
An improved optical fiber design has been found to exhibit a relatively low attenuation at the wavelength of 1385 nm (the “water peak”), allowing for Raman amplification to be efficient and effective at wavelengths in the S-band range of 1460 to 1530 nm. An ultra-dry process is…
Methods and apparatuses introduce mechanical twist to an optical fiber having relatively large polarization mode dispersion (PMD), such as unspun fiber or fiber spun with constant spatial frequency, which mechanical twist reduces the fiber's PMD. A spool of optical fiber…
Embodiments of the invention include a method for making optical fiber having reduced aging or hydrogen aging loss over the life of the fiber and optical fiber systems including such optical fibers. Improved silicon-oxygen stoichiometry during one or more preform manufacturing…
The specification describes an improved optical fiber design in which the criteria for high performance in a Raman amplified optical system, such as moderate effective area, moderate dispersion, low dispersion slope, and selected zero dispersion wavelength, are simultaneously…
Methods for modifying preform core ovality during and subsequent to the formation of an optical fiber preform. Prior to MCVD deposition on a starting tube, the outer diameter of the starting tube is altered by etching or a like process to modify its ovality. Additionally, after…
The specification describes an improved optical fiber design in which the criteria for high performance in a Raman amplified optical system, such as moderate effective area, moderate dispersion, low dispersion slope, and selected zero dispersion wavelength, are simultaneously…
The specification describes an improved optical fiber design in which the criteria for high performance in a Raman amplified optical system, such as moderate effective area, moderate dispersion, low dispersion slope, and selected zero dispersion wavelength, are simultaneously…