In a process for treating molten aluminium and its alloys prior to casting, the metal is agitated by any suitable means while maintained in an atmosphere free from hydrogen, water vapour or other hydrogen gas supplied to the space above the metal, the surface of the metal…
Daniel Hanson
In the process described in the parent Specification for refining aluminium and aluminium alloys prior to casting, by agitating them in a hydrogen-free atmosphere while treating the surface of the molten metal with a flux, the flux is modified by the inclusion of boron or…
A tin alloy consists of 2-14 per cent of antimony, 1-10 per cent of cadmium, and the remainder tin. The alloys may be heated to 140-175 DEG C. and cooled, followed or not by heating to between 180 DEG C. and the melting point, and cooling. In some cases there may be a third…
Tin alloys contain 1-15 per cent, preferably 4-6 per cent, of cadmium, and are heated to between 130 DEG C. and the melting-point and cooled quickly. They may afterwards be heated to not more than 130 DEG C., for example in boiling water. The alloys may be used in the form of…
390,930. Suspending curtains. HANSON, A. E., 27, Rafford Way, Bromley, Kent, and HANSON, D., Upton House, Haselor, Warwickshire. Feb. 25, 1932, No. 5642. [Class 52 (v).] A combined stop and retaining spring for curtain runners W is adjustably or fixedly mounted on the rail R. A…
541,055. Alloys; annealing. LOWINGER, V. A., HANSON, D., and WALPOLE, W. T. PELL-. June 12, 1940, No. 10256. [Classes 72 and 82 (i)] Tin alloys contain 7-20 per cent. of antimony and are subjected to rapid cooling between 200‹C. and the melting point followed by reheating at…