The invention relates to a powder made of polyoxymethylene (POM) for use in a selective laser sintering process, comprising the following parameters: isothermal crystallization time (at 152 °C) > 3 min, Mn 22000 - 25000 g/mol, Mw 60000 - 140000 g/mol, Mw/Mn 3 - 5, MVR 15 - 70…
Assignee / Organization
Dallner Claus
16Total Forward Citations
3Indexed Patents
5Avg Citations / Patent
3Portfolio H-Index
The invention relates to a polyoxymethylene (POM) powder for use in a selective laser sintering process and having the following parameters: Isothermal crystallization time (at 152° C.) >3 min Mn from 22 000 to 25 000 g/mol Mw from 60 000 to 140 000 g/mol Mw/Mn from 3 to 5…