High surface area iron material prepared from a low surface area iron metal precursor

A method for producing a high surface area iron material starting with a low surface area iron metal is disclosed. The iron material of the present invention has a surface area of at least about 200 m 2 /g, and is prepared via a method which comprises reacting a low surface area…

WO 03,097,236 A1#8997997 Most Cited · 11 citations0.5/yr · PR 2.93PendingWO · Application
Fischer-tropsch catalyst prepared with a high purity iron precursor

A Fischer-tropsch catalyst comprising iron and at least one promoter is prepared via a method which comprises the preparation of a high purity iron precursor and which uses a nominal amount of water in the catalyst production. The catalyst particles prepared with the high purity…

US 8,574,450 B2#21536515 Most Cited · 5 citations0.4/yr · PR 1.37ActiveUS · Utility
Method for preparing iron oxides
Inventors: Conca Esterino, Rubini Carlo, Petrini GuidoAssignee: Conca Esterino, Rubini CarloFiled 2011-05-24 · Granted 2013-11-05

Highly pure iron oxides are prepared by reaction of metallic iron, in the form of microspheroidal particles or of scraps or cuttings, with an agitated aqueous solution of a mono- or polycarboxylic acid with a pKa of 0.5 to 6 relative to the first carboxyl and capable of…

WO 2006/127261 A1#61477722 Most Cited · 1 citations0.1/yr · PR 0.75PendingWO · Application
High surface area iron material prepared from a low surface area iron metal precursor

A method for producing a high surface area iron material starting with a low surface area iron metal is disclosed. The iron material of the present invention has a surface area of at least about 200 m2/g, and is prepared via a method which comprises reacting a low surface area…

WO 2006/127261 B1#73039342 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
High surface area iron material prepared from a low surface area iron metal precursor

A method for producing a high surface area iron material starting with a low surface area iron metal is disclosed. The iron material of the present invention has a surface area of at least about 200 m2/g, and is prepared via a method which comprises reacting a low surface area…