The present invention relates to yarn dyeing, such as denim dyeing. A process provides a dyed yarn having reduced dye penetration and a white core at lower cost. The improved process for yarn dyeing is referred to herein as the CleanKore technology. The CleanKore technology…
Cleankore Llc
The present invention generally relates to sulfur dyeing of fabrics. In particular, a process is provided which provides a sulfur dyed yarn having reduced dye penetration and a white core. The process involves modification of existing sulfur dye ranges in order to more…
The invention generally relates to fabric dyeing, such as fabric dyeing using indigo or sulphur dyes. A process is provided which provides a dyed yarn having reduced dye penetration and a white core. The process involves modification of existing sulfur dye ranges to more…
A method of ring dyeing a yarn includes the steps of providing a cellulosic yarn chosen from the group consisting of open-end yarns and ring yarns. The yarn is immersed in only one sulfur dye box, the sulfur dye box having a sulfur concentration of 1 to 50 grams/liter. The yarn…
A method of ring dyeing a yarn comprises a series of steps, including providing a yarn chosen from the group consisting of open-end yarns and ring yarns. The yarn is immersed for between 7 to 40 seconds in a caustic bath having a caustic concentration of 50 to 175 g/l. The yarn…
The present invention relates to yarn dyeing, such as denim dyeing. A process provides a dyed yarn having reduced dye penetration and a white core at lower cost. The improved process for yarn dyeing is referred to herein as the CleanKore technology. The CleanKore technology…
The present invention generally relates to sulfur dyeing of fabrics. In particular, a process is provided which provides a sulfur dyed yarn having reduced dye penetration and a white core. The process involves modification of existing sulfur dye ranges in order to more…
A method of ring dyeing a yarn comprises a series of steps, including providing a yarn chosen from the group consisting of open-end yarns and ring yarns. The yarn is immersed for between 7 to 40 seconds in a caustic bath having a caustic concentration of 50 to 175 g/l. The yarn…
A method of ring dyeing a yarn includes the steps of providing a cellulosic yarn chosen from the group consisting of open-end yarns and ring yarns. The yarn is immersed in only one sulfur dye box, the sulfur dye box having a sulfur concentration of 1 to 50 grams/liter. The yarn…