The present invention relates to a process for producing a propylene terpolymer comprising comonomer units derived from ethylene and from one alpha-olefin selected from the group of C4-C8 alpha-olefins and being characterized by a total content of comonomer units not less than 8…
Cavalieri Claudio
Propylene polymers having specific values of total comonomer content and melting temperature, articles obtained therefrom, in particular extrusion blow molded articles, and gas-phase process for obtaining said propylene polymers.
A polyolefin composition comprising (percent by weight): A) from 7% to 19%; of a copolymer of propylene and 1 -hexenewherein said copolymer contains less than 1 % of recurring units derived from hexene-1; B) from 81% to 93% of a heterophasic polypropylene composition comprising:…
A propylene polymer composition comprising (weight percentages being referred to the sum of A+B): A propylene polymer composition comprising (weight percentages being referred to the sum of A+B): (A) 60-90% by weight of a copolymer of propylene with ethylene containing less than…
A propylene/ethylene/1-hexene terpolymer containing from 1.0 wt% to 2.5wt%, of ethylene derived units and from 2.0wt% to 4.0wt% of 1-hexene derived units, the sum of the amounts of propylene, ethylene and 1-.hexene derived units being 100, having the following features: a) the…
Random propylene/ethylene copolymers are provided characterized by Ethylene content in the range of 4.5-7%wt; Mw/Mn (via GPC) in the range 3.5-5.5; Mz/Mw (via GPC) lower than 4; absence of 2-1 regioinversion, and Melting Temperature (Tm) (non-nucleated grade) lower than 143°C.…
A process for the preparation of a propylene copolymer composition having a Flexural modulus lower than 500MPa, a total ethylene content higher than 9% and a Xylene soluble fraction at room temperature higher than 20% comprising at least one polymerization step carried out in a…
A polypropylene composition for injection-moulded drainage systems comprising 78-84 wt% of a crystalline propylene polymer, 8 to less than 13 wt% of an elastomeric copolymer and 8 to less than 13 wt% of polyethylene. The said composition exhibits a flexural modulus value higher…
A heterophasic polypropylene composition comprising (percent by weight referred to the sum of components A) and B)): A) from 80 % to 97 % of a random copolymer of propylene containing from 0.1 to 4 % of 1-hexene derived units; B) from 3-20 % of a copolymer of propylene and…
Use of propylene polymers having Polydispersity Index value P.I.(2) greater than or equal to 15 for the nucleation of polypropylene resins having a Polydispersity Index value P.I.(1) fulfilling the equation P.I.(2)-P.I.(1) ≥ 10.
Articles, particularly pressure pipes, having high strength as well as high stiffness and very good impact resistance even at low temperatures can be obtained by using a heterophasic polyolefϊn composition comprising (percent by weight) 70-90% of a random copolymer of propylene…
A propylene composition comprising (percent by weight): A) 60%-95%, of a crystalline propylene copolymer containing from 2.0% to 10.0% of ethylene derived units having a melting point ranging from 148°C to 160°C; wherein the melting temperature Tm is measured by DSC on the…
A polyolefin composition for pipes comprising (percent by weight): A) from 1% to 9.5%; of a copolymer of propylene and hexene-1 wherein said copolymer comprises from 0.1 to 5 % of recurring units derived from hexene-1; B) from 80.5% to 99% of a heterophasic polypropylene…
The present invention relates to a process for producing a propylene terpolymer comprising comonomer units derived from ethylene and from one alpha-olefin selected from the group of C 4 -C 8 alpha-olefins and being characterized by a total content of comonomer units not less…
A propylene/ethylene/1-hexene terpolymer containing from 1.0 wt% to 2.5 wt %, of ethylene derived units and from 2.0 wt % to 4.0 wt % of 1-hexene derived units, the sum of the amounts of propylene, ethylene and 1-.hexene derived units being 100, having the following features: a)…
A polyolefin composition for pipes comprising (percent by weight): A) from 1% to 9.5%; of a copolymer of propylene and hexene-1 wherein said copolymer comprises from 0.1 to 5% of recurring units derived from hexene-1; B) from 80.5% to 99% of a heterophasic polypropylene…
Wooden bathroom fittings like washbasins, baths, bidets, W.C. and shower bases are proposed which are obtained from wooden starting blocks (3) formed by a plurality of panels (1; 4) made by glueing together a number of strips (2; 6) the axis of which extends parallel to the…
A container comprising a polyolefin composition comprising: A) from 59 wt% to 84 wt%, of a propylene homopolymer having isotactic pentads (mmmm) measured with by 13 C-NMR higher than 96%, B) from 16 wt% to 41 wt%, of a copolymer of propylene and ethylene with from 30wt% to…
Polypropylene compositions, particularly suited for preparation of stretched/oriented articles, especially for injection stretch blow moulded bottles, comprising: A) one or more propylene homopolymers or propylene copolymers or their mixtures; B) from 500 to about 1500 ppm by…
A polypropylene composition for injection-moulded drainage systems comprising 78-84 wt % of a crystalline propylene polymer, 8 to less than 13 wt % of an elastomeric copolymer and 8 to less than 13 wt % of polyethylene. The said composition exhibits a flexural modulus value…
A polyolefin composition comprising (percent by weight): A) from 7% to 19%; of a copolymer of propylene and 1-hexene wherein said copolymer contains less than 1% of recurring units derived from hexene-1; B) from 81% to 93% of a heterophasic polypropylene composition comprising:…
A propylene polymer composition having a Flexural modulus lower than 500MPa, a total ethylene content from 9 to 30% by weight, a xylene soluble fraction at room temperature higher than 25% by weight, a melting temperature measured by DSC (Tm°C) from 130 to 150°C and a ratio…
A propylene composition comprising (percent by weight): A) 60%-95%, of a crystalline propylene copolymer containing from 2.0% to 10.0% of ethylene derived units having a melting point ranging from 148° C. to 160° C.; wherein the melting temperature Tm is measured by DSC on the…
A heterophasic polypropylene composition comprising (percent by weight referred to the sum of components A) and B)): A) from 80% to 97% of a random copolymer of propylene containing from 0.1 to 4% of 1-hexene derived units; B) from 3-20% of a copolymer of propylene and ethylene…
A propylene polymer composition comprising (percent by weight): A) 65%-85% of a propylene copolymer containing from 2.0% to 5.0% of ethylene derived units having MFR L (Melt Flow Rate according to ASTM 1238, condition L, i.e. 230° C. and 2.16 kg load) from 0.5 to 50 g/10 min and…