Low dielectric constant porous materials with improved elastic modulus. The process of making such porous materials involves providing a porous dielectric material and ultraviolet (UV) curing of the porous dielectric material to produce a UV cured porous dielectric material. UV…
Carlo Waldfried
Low dielectric constant porous materials with improved elastic modulus and film hardness. The process of making such porous materials involves providing a porous dielectric material and plasma curing the porous dielectric material to produce a plasma cured porous dielectric…
Low dielectric constant materials with improved elastic modulus and material hardness. The process of making such materials involves providing a dielectric material and ultraviolet (UV) curing the material to produce a UV cured dielectric material. UV curing yields a material…
A substantially oxygen-free and nitrogen-free plasma ashing process for removing photoresist in the presence of a low k material from a semiconductor substrate includes forming reactive species by exposing a plasma gas composition to an energy source to form plasma. The plasma…
A method of forming a coating on a substrate. A coating is formed on a substrate by depositing a solution comprising a resin molecule containing at least 2 Si—H groups, at least 2 Si—CH 3 groups, or a combination thereof, and, a solvent in a manner in which at least about 5…
Low dielectric constant films with improved elastic modulus. The method of making such coatings involves providing a porous network coating produced from a resin containing at least 2 Si—H groups and plasma curing the coating to convert the coating into porous silica. Plasma…
An oxygen-free and nitrogen-free plasma ashing process for removing photoresist in the presence of a low k material from a semiconductor substrate. The process includes forming reactive species by exposing a plasma gas composition to an energy source to form plasma. The plasma…
A process for removing polymers formed during etching and etch residues from a semiconductor substrate by exposing the substrate to plasmas of neutral chemistry. The plasma generates atomic hydrogen species and atomic oxygen species in about equal amounts that react with and…
Low dielectric constant film materials with improved elastic modulus. The method of making such film materials involves providing a porous methyl silsesquioxane based dielectric film material produced from a resin containing at least 2 Si—CH 3 groups and plasma curing the porous…
Low dielectric constant porous materials with improved elastic modulus and material hardness. The process of making such porous materials involves providing a porous dielectric material and plasma curing the porous dielectric material with a fluorine-free plasma gas to produce a…
A low temperature plasma ashing process for use with substrates comprising a ferroelectric material. The process generally includes plasma ashing the photoresist and residues at a temperature of about room temperature to about 140° C., wherein the plasma is generated from a gas…
A plasma ashing process and apparatus for selectively ashing photoresist and/or post etch residues from a semiconductor substrate includes generating a reduced ion density plasma in a plasma generation region at a pressure of at least 2 torr greater than the processing chamber…
Low dielectric constant porous materials with improved elastic modulus and film hardness. The process of making such porous materials involves providing a porous dielectric material and plasma curing the porous dielectric material with a fluorine-free plasma gas to produce a…
Low dielectric constant films with improved elastic modulus. An SiO 2 -containing plasma cured coating having a first dielectric constant and having a first elastic modulus is provided, the coating being formed by providing a porous network coating produced from a resin molecule…