An aluminum alloy product is provided that includes an ADC12-T4 aluminum alloy. The ADC12-T4 aluminum alloy is cast into the product utilizing a high pressure, slow velocity casting technique. Further, an alloy is provided that in some embodiments produces cast parts with high…
Brown Zach
A method for the refining of primary aluminum in hypoeutectic alloys by mixing a titanium based grain refiner into an Al-Si alloy. The method provides control of the morphology, size, and distribution of primary Al in a hypoeutectic Al-Si casting by mixing a hypoeutectic Al-Si…
A method for the refining of primary silicon in hypereutectic alloys by mixing at least two hypereutectic alloys into a solid/semi-solid hypereutectic slurry is described. The method provides control of the morphology, size, and distribution of primary Si in a hypereutectic…
A vehicle part formed at least in part of a blended material is provided. The blended material is formed by mixing an improved aluminum alloy and a recycled aluminum alloy. The recycled aluminum alloy can be obtained from road wheels. The blended alloy preferable meets the Aural…
An embodiment of the presently claimed invention includes an in-situ slurry formation apparatus mounted to die casting machines to convert liquid metal to semi-solid metal (SSM). Thus, there is no need to modify existing machines or change the cell layout to accommodate more…
To cast a part, an injectable form of an aluminum-copper (206) alloy is generated and the aluminum-copper (206) alloy is injected into a mold. This mold corresponds to the part. In addition, the aluminum-copper (206) alloy is solidified to generate the part and the part is…
An apparatus and method are provided that increase yield and reduce cycle time. In particular, a gate plate for a die casting machine is configured to lessen the waste produced during die casting, resulting in greater yield. Further, the gate plate is configured with tapered…
A method for the refining of primary aluminum in hypoeutectic alloys by mixing at least two hypoeutectic alloys into a solid/semi-solid hypoeutectic slurry is described. The method provides control of the morphology, size, and distribution of primary Al in a hypoeutectic Al-Si…
A method for the refining of primary aluminum in hypoeutectic alloys by mixing at least two hypoeutectic alloys into a solid/semi-solid hypoeutectic slurry is described. The method provides control of the morphology, size, and distribution of primary Al in a hypoeutectic Al-Si…
A method for the refining of primary aluminum in hypoeutectic alloys by mixing a titanium based grain refiner into an Al-Si alloy. The method provides control of the morphology, size, and distribution of primary Al in a hypoeutectic Al-Si casting by mixing a hypoeutectic Al-Si…
To cast a part, an injectable form of an aluminum-copper (206) alloy is generated and the aluminum-copper (206) alloy is injected into a mold. This mold corresponds to the part. In addition, the aluminum-copper (206) alloy is solidified to generate the part and the part is…
An aluminum alloy product is provided that includes an ADC12-T4 aluminum alloy. The ADC12-T4 aluminum alloy is cast into the product utilizing a high pressure, slow velocity casting technique. Further, an alloy is provided that in some embodiments produces cast parts with high…
An aluminum alloy product is provided that includes an ADC12-T4 aluminum alloy. The ADC12-T4 aluminum alloy is cast into the product utilizing a high pressure, slow velocity casting technique. Further, an alloy is provided that in some embodiments produces cast parts with high…
An improved aluminum alloy for casting into a component, such as a vehicle component, is provided. The improved aluminum alloy includes at least 80 wt. % aluminum; 6.0 to 8.0 wt. % silicon; 1.0 to 2.0 wt. % zinc; 0.10 to 0.6 wt. % magnesium; 0.1 to 0.60 wt. % copper; 0.20. to…
An improved aluminum alloy for casting into a component, such as a vehicle component, is provided. The aluminum alloy preferably includes at least 80 weight percent (wt. %) aluminum; 9.5 to 11.5 wt. % silicon; 1.5 max wt. % zinc; 0.1 wt. % to 0.6 wt. % magnesium; 0.10 wt. % to…