The chemically resistant borosilicate glass has the following composition (in % by weight): SiO 2 , 67-74; B 2 O 3 , 5-10; Al 2 O 3 , 3-10; Li 2 O, 0-4; Na 2 O, 0-10; K 2 O, 0-10; MgO, 0-2; CaO, 0-3; SrO, 0-3; BaO, 0-3; ZnO, 0-3; ZrO 2 , 0-3; CeO 2 , 0-1; with ΣLi 2 O+Na 2 O+K 2…
Assignee / Organization
Brigitte Hueber
77Total Forward Citations
3Indexed Patents
26Avg Citations / Patent
3Portfolio H-Index
The method for making UV-absorbing glass, which transmits in a visible range, includes melting raw materials to form a melt and producing the melt under oxidative conditions. The melt has the following composition (in % by weight): SiO 2 , 55-79; B 2 O 3 , 3-25; Al 2 O 3 , 0-10;…
The lamp bulb for discharge lamps is made from an aluminosilicate glass with a transformation temperature Tg>600° C. The aluminosilicate glass has a composition (in % by weight, based on oxide content) of SiO 2 >55-64; Al 2 O 3 , 13-18; B 2 O 3 , 0-5.5; MgO, 0-7; CaO,…