Transparent and impact-resistant crosslinked acrylic composition constituted of a brittle matrix (I) having a glass transition temperature of greater than 0°C, and elastomeric domains having a characteristic dimension of less than l00 nm constituted by macromolecular sequences…
Bourrigaud Sylvain
The present invention relates to pulverulent compositions based on carbon nanotubes, which exhibit excellent dispersibility in polymeric materials and advantageously can be used as reinforcements and/or modifiers of conducting and/or thermal properties. They can easily be…
Transparent and impact-resistant crosslinked acrylic composition consisting of a brittle matrix (I) having a glass transition temperature of greater than 0° C. and of elastomeric domains having a characteristic dimension of less than 100 nm consisting of macromolecular sequences…
The invention concerns a clear composition filtering near infrared radiation comprising by weight: 70 to 99.9 parts of at least one methacrylic polymer; 0.1 to 30 parts of at least one impact modifier in the form of multilayer particles; 0.0001 to 1 part of at least one…
Transparent and impact-resistant crosslinked acrylic composition consisting of a brittle matrix (I) having a glass transition temperature of greater than 0° C. and of elastomeric domains having a characteristic dimension of less than 100 nm consisting of macromolecular sequences…
The invention relates to a composition that contains, in weight and for a total of 100%: from 10 to 40% of a block copolymer including a central block B with Tg<0° C. and at least two side rigid blocks A and A′ with Tg>0° C. that include MAM as a main monomer as well as…
The invention relates to a composition that contains, in weight and for a total of 100 % : from 10 to 40 % of a block copolymer including a central block B with Tg<0°C and at least two side rigid blocks A and A' with Tg>0°C that include MAM as a main monomer as well as…
The invention relates to a block copolymer comprising: • at least one soft block A having a T g between -55°C and 0°C, preferably between -40°C and -1°C and • at least one block B comprising at least one photoactive monomer bearing a photoisomerizable chromophore. The…