Patents
Assignee / Organization

Bortinger Arie

50Total Forward Citations
9Indexed Patents
6Avg Citations / Patent
3Portfolio H-Index
US 8,378,129 B2#3784483 Most Cited · 22 citations1.7/yr · PR 1.62ActiveUS · Utility
Two-stage calcination for catalyst production
Inventors: Bhise Vijay S, Bortinger Arie, Allen Stephen RAssignee: Sd Lizenzverwertungsgesell Mbh, Bhise Vijay SFiled 2011-10-25 · Granted 2013-02-19

The invention relates to an improved process for producing a catalyst useful for the epoxidation of ethylene to ethylene oxide. In forming the catalyst, a silver-impregnated support is subjected to two calcinations. The support is subjected to a first calcination in a first…

US 8,546,297 B2#4358145 Most Cited · 20 citations1.5/yr · PR 1.66ActiveUS · Utility
Method for preparing an epoxidation catalyst
Inventors: Rokicki Andrzej, Bortinger Arie, Verrier ChristelleAssignee: Rokicki Andrzej, Bortinger ArieFiled 2011-05-17 · Granted 2013-10-01

A process for the preparation of a catalyst useful for the vapor phase production of ethylene oxide from ethylene and oxygen comprising the steps of providing a catalyst precursor comprising an inert support having a catalytically effective amount of a silver containing…

US 8,097,557 B2#27372119 Most Cited · 4 citations0.3/yr · PR 1.01ActiveUS · Utility
Two-stage calcination for catalyst production
Inventors: Bhise Vijay S, Bortinger Arie, Allen Stephen RAssignee: Bhise Vijay S, Bortinger ArieFiled 2006-08-08 · Granted 2012-01-17

The invention relates to an improved process for producing a catalyst useful for the epoxidation of ethylene to ethylene oxide. In forming the catalyst, a silver-impregnated support is subjected to two calcinations. The support is subjected to a first calcination in a first…

US 2012041217 A1#40701704 Most Cited · 2 citations0.1/yr · PR 0.99PendingUS · Application
Two-stage calcination for catalyst production

The invention relates to an improved process for producing a catalyst useful for the epoxidation of ethylene to ethylene oxide. In forming the catalyst, a silver-impregnated support is subjected to two calcinations. The support is subjected to a first calcination in a first…

WO 2004/103557 A1#61606765 Most Cited · 1 citations0.1/yr · PR 0.75PendingWO · Application
Phoshorus/vanadium catalyst preparation

A process for preparing a catalyst for maleic anhydride production wherein a +5 vanadium compound such as , an anhydrous phosphonic acid, and optionally promoters are admixed in an organic alcohol solvent, the admixture is rapidly brought to reflux and thereafter refluxed to…

WO 2011/146426 A2#60627974 Most Cited · 1 citations0.1/yr · PR 0.76PendingWO · Application
Method for preparing an epoxidation catalyst

A process for the preparation of a catalyst useful for the vapor phase production of ethylene oxide from ethylene and oxygen comprising the steps of providing a catalyst precursor comprising an inert support having a catalytically effective amount of a silver containing…

US 2011301367 A1#114614800 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Method for preparing an epoxidation catalyst

A process for the preparation of a catalyst useful for the vapor phase production of ethylene oxide from ethylene and oxygen comprising the steps of providing a catalyst precursor comprising an inert support having a catalytically effective amount of a silver containing…

WO 2011/146426 A3#107851410 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Method for preparing an epoxidation catalyst

A process for the preparation of a catalyst useful for the vapor phase production of ethylene oxide from ethylene and oxygen comprising the steps of providing a catalyst precursor comprising an inert support having a catalytically effective amount of a silver containing…

WO 9,704,866 A1#64299397 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Phosphorus/vanadium catalyst preparation
Inventors: Bortinger ArieAssignee: Bortinger ArieFiled 1995-07-28

A vanadium/phosphorus mixed oxide catalyst containing not more than 0.2 wt.% chloride is produced by drying chloride containing catalyst precursor at 100-180 °C, calcining the dried precursor, preferably under nitrogen, at 200-300 °C and activating the calcined precursor at…