Patents
GB 621,224 A#14118052 Most Cited · 7 citations0.1/yr · PR 4.68ExpiredGB · Utility
Working and heat-treating beryllium-copper alloys
Inventors: Assignee: Beryllium CorpFiled 1946-08-23

In a method of working cold workable-precipitation hardenable beryllium copper alloys to enable them to be repeatedly cold-worked and recrystallized by heating to 750 DEG to 1040 DEG F., the solution annealed cold-worked alloy is heat treated at 750 DEG to 1060 DEG F. for at…

US 3,724,050 A#14375549 Most Cited · 7 citations0.1/yr · PR 2.56ExpiredUS · Utility
Method of making beryllium shapes from powder metal
Inventors: Velten E, Jagaciak G, Wambold J, Epstein AAssignee: Beryllium CorpFiled 1968-09-19 · Granted 1973-04-03

A method of making beryllium or beryllium alloy shapes from powder metal by first pressing the beryllium or beryllium alloy shape either by isostatic pressing or conventional mechanical compacting methods at room temperature to 60 percent to 95 percent of theoretical density at…

GB 1,056,825 A#23848805 Most Cited · 4 citations0.1/yr · PR 1.54ExpiredGB · Utility
Production of beryllium hydroxide
Inventors: J Morana Simon, Simons Gordon F, J Wummer CarlAssignee: Beryllium CorpFiled 1963-10-28

Commercial beryllium hydroxide is purified by forming therefrom a solution containing beryllium sulphate and impurities other than silica and alkaline each metal fluorides, adding to the solution a chelating agent to retain in solution the said impurities and adding ammonium…

GB 1,066,024 A#24526579 Most Cited · 4 citations0.1/yr · PR 1.41ExpiredGB · Utility
Production of beryllium hydroxide

Impure beryllium hydroxide is purified by treating it with 10 to 50% excess concentrated sulphuric acid, heating the mixture at above 300 DEG F., diluting with deionized water to a concentration of 50 g. BeO per litre, filtering off silica, alkaline earth metal fluorides and…