Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (M w /M n ) from about 2 to about 30, a melt index (I 2 ) from about 0.1 to about 50 grams per 10 minutes, and further…
Berbee Otto
The invention provides an ethylene-based polymer comprising the following properties: a) a melt index (12)>2.0 dg/min; b) a Mw(abs) versus 12 relationship: Mw(abs)<A+B(I2), where A=2.40×10 5 g/mole, and B=−8.00×10 3 (g/mole)/(dg/min); and c) a G′ versus 12 relationship:…
Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (M w /M n ) from about 2 to about 30, a melt index (I 2 ) from about 0.1 to about 50 grams per 10 minutes, and further…
A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone operating at polymerization conditions to produce a…
A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising ethylene and optionally a chain transfer agent system (CTA system) into a first autoclave reactor zone operating at polymerization conditions to…
The invention provides a high pressure polymerization process to form an ethylene-based polymer, the process comprising at least the following steps: feeding ethylene to a first reaction zone and to one or more subsequent reaction zones, and wherein for each subsequent reaction…
The invention provides an ethylene-based polymer comprising the following properties: A) a “weight fraction (w) of molecular weight greater than 106 g/mole, based on the total weight of polymer, and as determined by GPC(abs),” that meets the following relationship: w<A+B(I2),…
The invention provides an ethylene-based polymer comprising the following properties: a) a melt index (12)>2.0 dg/min; b) a Mw(abs) versus 12 relationship: Mw(abs)<A+B(I2), where A=2.40×10 5 g/mole, and B=−8.00×10 3 (g/mole)/(dg/min); and c) a G′ versus 12 relationship:…
Ethylene-based interpolymers, e.g., ethylene-acrylic acid copolymers, are made by a process comprising the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone to produce a first zone reaction…
The instant invention is a free radical initiator system, and a high pressure, free radical polymerization process for producing a low density polyethylene polymer. The free radical initiator system according to instant invention includes at least one peroxide initiator, at…
Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (M w /M n ) from about 2 to about 30, a melt index (I 2 ) from about 0.1 to about 50 grams per 10 minutes, and further…
Ethylene-based interpolymers, e.g., ethylene-acrylic acid copolymers, are made by a process comprising the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone to produce a first zone reaction…
The present invention provides an injection nozzle for mixing an initiator with a process fluid. Then injection nozzle comprises a body comprising an inlet port, and outlet port, and an injector inlet; a process fluid flow passage; an initiator flow fluid passage; and a stylus.…
A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising ethylene and optionally a chain transfer agent system (CTA system) into a first autoclave reactor zone operating at polymerization conditions to…
A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone operating at polymerization conditions to produce a…
A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising ethylene and optionally a chain transfer agent system (CTA system) into a first autoclave reactor zone operating at polymerization conditions to…
A high pressure polymerization process to form an ethylene-based polymer comprises the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone operating at polymerization conditions to produce a…
Ethylene-based interpolymers, e.g., ethylene-acrylic acid copolymers, are made by a process comprising the steps of: A. Injecting a first feed comprising a chain transfer agent system (CTA system) and ethylene into a first autoclave reactor zone to produce a first zone reaction…
The invention relates to a method for producing ethylene homopolymerizates and ethylene copolymerizates exhibiting a lower mass density of up to 0.930 g/cm3 and a melt index ranging from 0.15 to 25 g/10 min (2,16 kg; 463 K). Said polymerizates exhibit an improved processing…
The instant invention is a free radical initiator system, and a high pressure, free radical polymerization process for producing a low density polyethylene polymer. The free radical initiator system according to instant invention includes at least one peroxide initiator, at…
An initiator injection nozzle for mixing an initiator with a process fluid, comprising: a body comprising an inlet port to receive the process fluid, an outlet port, and an injector inlet to receive initiator; a process fluid flow passage through which the process fluid…
A polymer comprises units derived from ethylene and polyalkylene, the polymer having at least 0.15 units of amyl groups per 1000 carbon atoms as determined by 13C Nuclear Magnetic Resonance (NMR).
A process for producing an ethylene-based polymer comprises polymerizing, by the presence of at least one free-radical initiator and using a high pressure tubular polymerization process, a reaction mixture containing ethylene and at least one CTA system comprising one or more…
A polymer comprises units derived from ethylene and poly(alkoxide) the polymer having at least 0.15 units of amyl groups per 1000 carbon atoms as determined by 13C Nuclear Magnetic Resonance (NMR).
A polymer comprises units derived from ethylene and poly(alkoxide) the polymer having at least 0.15 units of amyl groups per 1000 carbon atoms as determined by 13C Nuclear Magnetic Resonance (NMR).