A method of treating a catalyst support comprises introducing onto and/or into an untreated catalyst support which is partially soluble in an aqueous acid solution and/or a neutral aqueous solution, Si, Zr, Cu, Zn, Mn, Ba, Co, Ni and/or La as a modifying component. The modifying…
Barradas Sean
A process for producing a clean wax product includes contacting, at an elevated temperature between 180°C and 250°C and at an elevated pressure between 10 bar and 40 bar, a synthesis gas comprising hydrogen and carbon monoxide with a cobalt slurry phase Fischer-Tropsch synthesis…
A method of treating an untreated catalyst support includes contacting an untreated catalyst support which is partially soluble in an aqueous acid and/or a neutral aqueous solution with a modifying component precursor of the formula Me(OR)x where Me is a modifying component…
A process for preparing a catalyst precursor comprises subjecting, in an initial treatment stage, a slurry of a catalyst support, an active catalyst component precursor, and water, to treatment at elevated temperature and at sub-atmospheric pressure, to impregnate the support…
A process for preparing a cobalt-containing hydrocarbon synthesis catalyst precursor includes calcining a loaded catalyst support comprising a catalyst support supporting a cobalt compound. The calcination includes heating the loaded catalyst support over a heating temperature…
A method of preparing a catalyst precursor comprises contacting a catalyst support material with a tungsten compound, to obtain a tungsten-containing catalyst support material. The tungsten-containing catalyst support material is calcined at a temperature above 900° C. to obtain…
A method of preparing a catalyst precursor comprises contacting a catalyst support material with a tungsten compound, to obtain a tungsten-containing catalyst support material. The tungsten-containing catalyst support material is calcined at a temperature above 900°C to obtain a…
A method of preparing a catalyst precursor comprises contacting a catalyst support material with a tungsten compound, to obtain a tungsten-containing catalyst support material. The tungsten-containing catalyst support material is calcined at a temperature above 900° C. to obtain…
A method of treating an untreated catalyst support includes contacting an untreated catalyst support which is partially soluble in an aqueous acid and/or a neutral aqueous solution with a modifying component precursor of the formula Me(OR)x where Me is a modifying component…
A process for producing a clean wax product includes contacting, at an elevated temperature between 180°C and 250°C and at an elevated pressure between 10 bar and 40 bar, a synthesis gas comprising hydrogen and carbon monoxide with a cobalt slurry phase Fischer-Tropsch synthesis…
A process for preparing a cobalt-containing hydrocarbon synthesis catalyst precursor includes calcining a loaded catalyst support comprising a catalyst support supporting a cobalt compound. The calcination includes heating the loaded catalyst support over a heating temperature…