There are described components of a steam turbine, comprising a thermally insulating layer and a metallic anti-erosion layer on said thermally insulating layer. The anti-erosion layer is provided with the same material as the metallic connecting layer.
Barnikel Jochen
The invention relates to components (333, 366) of a steam turbine (300, 303), comprising a thermally insulating layer (7) and a metallic anti-erosion layer (13) on said thermally insulating layer (7). The anti-erosion layer (13) is provided with the same material as the metallic…
The invention relates to a component having a coating system, which comprises at least one bonding coat applied directly onto the component and at least one thermal barrier coat formed on the bonding coat, the bonding coat comprising from 22 to 36 wt. % Cr, from 15 to 30 wt. %…
The invention relates to a method for reducing biological contaminants in a water-bearing system (3) that contains an installation part susceptible to corrosion (19). To reduce the biological contaminant, a biocide (11) is added to the water-bearing system (3). The concentration…
The invention relates to a component having a coating system, which comprises at least one bonding coat applied directly onto the component and at least one thermal barrier coat formed on the bonding coat, the bonding coat comprising from 22 to 36 wt. % Cr, from 15 to 30 wt. %…
The invention relates to the use of thermal insulation layers (7) on steam power plant components and substantially comprises an adhesive layer and/or an erosive protection layer (13), having similar or the same thermal expansion coefficients compared to a base material (4) or…
The invention relates to a component having a coating system, which comprises at least one bonding coat applied directly onto the component and at least one thermal barrier coat formed on the bonding coat, the bonding coat comprising from 22 to 36 wt. % Cr, from 15 to 30 wt. %…
The invention relates to a method for producing a turbine component, comprising the following steps: applying a spray coating (14) to the surface of a mold (10) and pouring the casting material (18) into said mold (10) in such a manner as to produce a permanent connection…
The invention relates to a method for producing a turbine component, comprising the following steps: applying a spray coating (14) to the surface of a mold (10) and pouring the casting material (18) into said mold (10) in such a manner as to produce a permanent connection…
The invention relates to a method for repairing a component (1), particularly steam turbine component, particularly an inner housing or outer housing and a valve body (1) of a steam turbine. According to the invention, the method is characterized by a protective layer being…
The invention relates to a method for producing a layer on a turbine component, wherein the turbine component consists of a ferritic base material, bonded to which is a thermal barrier coating, which is bonded on the ferritic base material by means of a bonding layer, wherein…