A hydrocarbon polymer modifier (HPM) having high softening point and high aromaticity, is an interpolymer of (i) a piperylene component; (ii) an aromatic component; and (iii) a cyclic pentadiene component comprising a dicyclopentadiene fraction (DCPD fraction) and a…
Barbee Thomas R
Provided are elastomeric compositions comprising at least one elastomer and a hydrocarbon polymer additive. Preferably the hydrocarbon polymer additive comprises from 60 to 90% piperylene, from 5 to 15% cyclic components, from 5 to 20% styrenic components, up to 5% isoprene, up…
A hydrocarbon polymer modifier (HPM) having high softening point and high aromaticity, is an interpolymer of (i) a piperylene component; (ii) an aromatic component; and (iii) a cyclic pentadiene component comprising a dicyclopentadiene fraction (DCPD fraction) and a…
An elastomeric composition incorporating a hydrocarbon polymer modifier including piperylene, cyclic pentadiene and aromatic components, and having a softening point from 80° C. to 160° C., z-average molecular weight greater than 10,000, and at least 1 mole percent aromatic…
An elastomeric composition incorporating a hydrocarbon polymer modifier including piperylene, cyclic pentadiene and aromatic components, and having a softening point from 80° C. to 160° C., z-average molecular weight greater than 10,000, and at least 1 mole percent aromatic…
A hydrocarbon polymer modifier (HPM) having high softening point and high aromaticity, is an interpolymer of (i) a piperylene component; (ii) an aromatic component; and (iii) a cyclic pentadiene component comprising a dicyclopentadiene fraction (DCPD fraction) and a…
Provided are elastomeric compositions comprising at least one elastomer and a hydrocarbon polymer additive. Preferably the hydrocarbon polymer additive comprises from 60 to 90% piperylene, from 5 to 15% cyclic components, from 5 to 20% styrenic components, up to 5% isoprene, up…
An elastomeric composition incorporating a hydrocarbon polymer modifier including piperylene, cyclic pentadiene and aromatic components, and having a softening point from 80°C to 160°C, z-average molecular weight greater than 10,000, and at least 1 mole percent aromatic…
High strength presulfided catalyst for hydrogenating hydrocarbon resins without an in situ sulfiding step. The catalyst particles have a supported metal catalyst structure with presulfided interstitial surfaces with about 20 weight percent of a low molecular weight hydrocarbon…