The (ingot) mould according to the invention is provided with a thermo-insulating hot top (2) made from rigid refractory material implanted on the tube element made from chilled copper (1) and means (8, 18, 12, 12, 13, 10) are provided for injecting, through the wall, a…
Ascometal Sa
The invention relates to a method for fabricating a piece of structural steel that includes thermal or thermomechanical treatment steps that could ordinarily lower the fatigue strength and shock and impact resistance of the steel piece. In the method of the invention a workpiece…
The invention relates to a steel and to a process for the manufacture of a steel component formed by cold plastic deformation.
A process for manufacturing a forged connecting rod of the type including a big end, a shank and a small end. A connecting rod rough forging, free of lateral flash and including at least one bore initiator on the big end and on the small end, is manufactured by forging. The…
The fabrication of a monolithic piston for an internal combustion engine involves reheating of a blank to an intermediate temperature between the solidus and liquidus temperatures and forming by thixotropic forging. An Independent claim is also included for a monolithic piston…
Steel chemical composition of which contains, by weight: 0.1%</=C</=0.4%; 1%</=Mn</=1.8%; 0.15%</=Si</=1.7%; 0%</=Ni</=1%; 0%</=Cr</=1.2%; 0%</=Mo</=0.3%; 0%</=V</=0.3%; Cu</=0.35%; optionally from 0.005% to 0.06% of aluminum,…
A spring steel with high fatigue resistance in air and in corrosive conditions and with high resistance to cyclic sag, having the composition in weight percent: C=0.45-0.70% Si=1.65-2.50% Mn=0.20-0.75% Cr=0.60-2% Ni=0.15-1% Mo=traces-1% V=0.003-0.8% Cu=0.10-1% Ti=0.020-0.2%…
A spring steel with high fatigue resistance in air and in corrosive conditions and with high resistance to cyclic sag, having the composition in weight percent: C=0.45-0.70% Si=1.65-2.50% Mn=0.20-0.75% Cr=0.60-2% Ni=0.15-1% Mo=traces-1% V=0.003-0.8% Cu=0.10-1% Ti=0.020-0.2%…
Steel useful for the manufacture of a separable mechanical component, whose chemical composition preferably comprises, by weight: 0.25%≦C≦0.75%, 0.2%≦Si≦1.5%, 0.1%≦Mn≦2%, 0%≦Ni≦1%, 0%≦Cr≦1%, 0%≦Mo≦1%, 0%≦Cu≦1%, 0%≦V≦0.2%, 0.02%≦S≦0.35%, 0.04%≦P≦0.2%, 0%≦Al≦0.005%,…
Steel for the manufacture of a component for bearings, the chemical composition of which comprises, by weight: 0.6%<=C<=1.5%; 0.4%<=Mn<=1.5%; 0.75%<=Si<=2.5%; 0.2%<=Cr<=2%; 0%<=Ni<=0.5%; 0%<=Mo<=0.2%; 0%<Al<=0.05%; S<=0.04%; the…
A facility for hot forging workpieces starting from bars (2), which includes a device (8) for heating the bars (2), a device (3) for longitudinally moving the bars, a shearing machine (9) cutting hot billets to a length l, and a stop (11) for setting the billet length and a…
The invention relates to a method for producing, by forging by means of press tools, a connecting rod including a shank (3') and a small end (2') and a big end (4') forming bearings, the said connecting rod being made up of two substantially similar parts (10',…
A steel section comprises by weight 0.06-0.11% carbon, 1-1.7% manganese, 0.15-0.40% silicon, 0.025-0.10% sulphur, up to 0.025% phosphorous, 0-0.25% nickel, 0.5-1.2% chromium, 0.08-0.13% molybdenum, 0-0.25% copper, 0.003-0.035% aluminium, 0-0.035% titanium, 0-0.10% vanadium,…
Steel for the manufacture of forgings having a bainitic structure and the mechanical properties of which are: R p0 .2 ≧800 MPa, R m ≧1000 MPa, K cu ≧50 J/cm 2 its chemical composition comprising, by weight: 0.05%≦C≦0.12%, 0.1%≦Si≦0.45%, 1.01%≦Mn≦1.8%, 0.15%≦Cr ≦1.15%,…
Steel for the manufacture of a component for bearings, the chemical composition of which comprises, by weight: 0.6%</=C</=1.5%; 0.4%</=Mn</=1.5%; 0.75%</=Si</=2.5%; 0.2%</=Cr</=2%; 0%</=Ni</=0.5%; 0%</=Mo</=0.2%; 0%<Al</=0.05%;…
The invention provides a method of fabricating a steel part by forging, the method being characterized by the following steps: preparing and casting a steel having the following composition in percentages by weight: 0.06%<=C<=0.35%; 0.5%<=Mn<=2%;…
Steel for forging comprises by weight 0.05-0.12 (0.05-0.08)%, carbon, 0.1-0.45 (0.15-0.35)% Si, 1.01-1.8 (1.01-1.35)% Mn, 0.15-1.15 (0.8-1.15)% Cr, 0.06-0.12 (0.08-0.11)% Mo, up to 0.30% each of copper and nickel, 0.01-0.04% titanium, 0.005-0.04% aluminium, 0.006-0.013%…
A novel carburising or carbonitriding steel has the composition (by wt.) 0.2-0.26% C, 0.05-0.5% Si, 1 to less than 1.6% Mn, 0.4-1.5% Cr, 0.08 to less than 0.27% Mo, 0 to less than 0.6% Ni, 0.003-0.06% Al, 0-0.3% Cu, 0-0.1% S, less than 0.03% P, optionally up to 0.02% Te, up to…
A mechanical steel part in steel with high characteristics, characterized in that its composition, comprising in weight percentages, is 0.05%≦C≦0.25%; 1.2%≦Mn≦2%; 1%≦Cr≦2.5%; wherein the contents of C, Mn and Cr are such that (830-270C %-90 Mn %-70Cr %)≦560; 0<Si≦1.55;…
Mechanical part made of steel having high properties and process for manufacturing same. Mechanical part made of steel having high properties, characterized in that its composition, in percentages by weight, is: 0.05% ≤ C ≤ 0.25%; 1.2% ≤ Mn ≤ 2%; 1% ≤ Cr ≤ 2.5%; (830 - 270 C% -…
This invention relates to steel for forging, comprises by weight 0.1-0.4% carbon, 1-1.8% manganese, 0.15-1.7% silicon and up to 1% nickel, 1.2% chromium, 0.3% molybdenum, 0.3% vanadium and 0.35% copper. Optional ingredients are 0.005-0.06% aluminium, 0.0005-0.01% boron,…
The (ingot) mould according to the invention is provided with a thermo-insulating hot top (2) made from rigid refractory material implanted on the tube element made from chilled copper (1) and means (8, 18, 12, 12, 13, 10) are provided for injecting, through the wall, a…
The ingot mould according to the invention is provided with a heat-insulating hot top (2) made from rigid refractory material installed above the cooled copper tubular element (1) and means are provided for introducing, into the casting space, a lubricating fluid, at the base of…
A piston for an internal combustion engine is formed from a metal part cast in one piece. Heating of a billet is carried out so as to bring it to an intermediate temperature between its solidus temperature and its liquidus temperature, and shaping thereof by thixoforging is…
Elongate product such as a wire or a rod for the manufacture by cold forming, especially by cold coining, of wrought products which have a tensile strength higher than 1000 MPa and lower than 1170 MPa and an elasticity limit higher than 900 MPa. The elongate product is made of a…