Prepare extruded polymer foam comprising at least 50 weight-percent alkenyl aromatic polymer, a brominated flame retardant providing 0.8 to 1.4 weight percent bromide, 0.05 to 0.5 weight-percent hydrobromic acid scavenger, at least 1.5 weight-percent graphite and less than 0.1…
Arrowsmith David R
Extruded polymer foams are prepared using brominated fatty acids, an ester, amide or ester-amide of a brominated fatty acid, a glyceride of one or more brominated fatty acids, or a polymerized brominated fatty acid as an FR additive. The brominated FR additives unexpectedly are…
Extruded polymer foams are prepared using brominated fatty acids, an ester, amide or ester-amide of a brominated fatty acid, a glyceride of one or more brominated fatty acids, or a polymerized brominated fatty acid as an FR additive. The brominated FR additives unexpectedly are…
Extruded polymer foams are prepared using brominated fatty acids, an ester, amide or ester-amide of a brominated fatty acid, a glyceride of one or more brominated fatty acids, or a polymerized brominated fatty acid as an FR additive. The brominated FR additives unexpectedly are…
Extruded polymer foams are prepared using brominated fatty acids, an ester, amide or ester-amide of a brominated fatty acid, a glyceride of one or more brominated fatty acids, or a polymerized brominated fatty acid as an FR additive. The brominated FR additives unexpectedly are…
Prepare extruded polymer foam comprising at least 50 weight-percent alkenyl aromatic polymer, a brominated flame retardant providing 0.8 to 1.4 weight percent bromide, 0.05 to 0.5 weight-percent hydrobromic acid scavenger, at least 1.5 weight-percent graphite and less than 0.1…