In a method for producing a salt core for casting formed by a molten salt made of a salt mixture containing sodium salt, first, a melt is formed by heating a salt mixture. Next, a mold for core molding is heated to a temperature higher than about 0.52×Tm and lower than about…
Anzai Koichi
An object is to provide an electromagnetic stirrer that can provide an excellent stirring force more than before. An electromagnetic stirrer has a vertical electromagnetic field generating coil ( 1 ) vertically and circumferentially provided on the outer side of a container ( 5…
When a salt core (2) is formed by die casting, a melt is obtained first by heating and melting a mixed salt containing at least a potassium salt and a sodium salt. Then, the temperature of the melt is decreased to have the melt in a semi-solidified (solid-liquid coexisting)…
A salt core (2) is formed by casting a mixed material of a salt material and a ceramic material. Any one of a chloride, bromide, carbonate, and sulfate of potassium or sodium is used as the salt material. As the ceramic material, granular one having a density falling within a…
A salt core ( 2 ) is formed by casting a mixed material of a salt material and a ceramic material. Any one of a chloride, bromide, carbonate, and sulfate of potassium or sodium is used as the salt material. As the ceramic material, granular one having a density falling within a…
<P>PROBLEM TO BE SOLVED: To provide a method of preparing semi-solid slurry, which can easily prepare semi-solid slurry or a semi-solid molding in a short time without being restricted to a type/composition of a target metal, and a semi-solid molding. <P>SOLUTION:…
A salt core (2) prepared by casting a mixed material from a salt material and a ceramic material, wherein one of chlorides, bromides, carbonates and sulfates of potassium and sodium is used as the salt material, and the ceramic material is a particulate material having a density…
PROBLEM TO BE SOLVED: To shorten calculation time and to obtain the necessary information to the design of a metallic die by reducing calculating quantity to the metallic die for a die casting, etc., as a periodic heating and cooling system. SOLUTION: The shape of the metallic…
An object is to provide an electromagnetic stirrer that can provide an excellent stirring force more than before. An electromagnetic stirrer has a vertical electromagnetic field generating coil ( 1 ) vertically and circumferentially provided on the outer side of a container ( 5…
Disclosed is a salt core (2) composed of potassium and sodium as cations and chlorine and carbonic acid as anions. In the salt core (2), the molar ratio of the potassium ions in the total cations, namely XK+ (= [K+]/([Na+] + [K+]) x 100) is set at 60-70 mol%, and the molar ratio…
An electromagnetic stirrer which enables to obtain an excellent stirring force than the conventional stirrers. The electromagnetic stirrer comprises a coil (1) for generating a vertically traveling magnetic field provided on the outer circumference of a container (5) along the…
A salt core (2) is formed by casting a mixed material of a salt material and a ceramic material. Any one of a chloride, bromide, carbonate, and sulfate of potassium or sodium is used as the salt material. As the ceramic material, artificially synthesited cohislievs of any one of…
<P>PROBLEM TO BE SOLVED: To provide an Ni based alloy in which macro componential segregation can be suppressed as far as possible by controlling a cast structure with a trace amount of inclusions, and to provide a method for producing the same. <P>SOLUTION:…
A salt core (2) is formed by casting a mixed material of a salt material and a ceramic material. Any one of a chloride, bromide, carbonate, and sulfate of potassium or sodium is used as the salt material. As the ceramic material, artificially synthesited cohislievs of any one of…
There are provided manufacture of semi-solid slurry which can easily manufacture semi-solid slurry or a semi-solid molding in a short time without being restricted to a type/composition of a target metal, and a semi-solid molding. It is characteristic that, when a metal in a…
A salt core (2) is formed by casting a mixed material of a salt material and a ceramic material. Any one of a chloride, bromide, carbonate, and sulfate of potassium or sodium is used as the salt material. As the ceramic material, artificially synthesited cohislievs of any one of…
<P>PROBLEM TO BE SOLVED: To provide an Ni-based alloy in which the macroscopic segregation of components can be suppressed as far as possible by controlling a cast structure with a trace amount of inclusions, and to provide a method for producing the same.…
Disclosed is a salt core (2) which is formed into a shape of a water jacket (6) by die-casting or the like by using a salt of bromine and at least one of sodium and potassium and a salt of carbonic acid and at least one of sodium and potassium. The salt core (2) contains at…
First, a mixed salt is heated to produce a melt (S101). Next, a mold for core molding is heated to within a temperature range of 0.52 x Tm to 0.7 x Tm (S102). It should be noted that Tm is the liquidus temperature of the mixed salt expressed as an absolute temperature (K). Then…