High heat strength is imparted to low alloy pearlitic steels containing 0.6 per cent max. carbon, at least 0.7 per cent silicon and at least one of the following elements in the ranges given: 0.2 to 6 per cent chromium, 0.1 to 3 per cent molybdenum, 0.05 to 3 per cent vanadium,…
Assignee / Organization
Anton Robert Wagner
6Total Forward Citations
2Indexed Patents
3Avg Citations / Patent
1Portfolio H-Index
Key Inventors:
1,146,911. Continuous-casting machines. A. R. WAGNER. 24 March, 1966 [27 March, 1965], No. 13086/66. Heading B3F. A method of continuously casting molten metal comprises continually producing a substantially vertical tubular metallic envelope, pouring molten metal into the upper…