Compositions, methods and systems for manufacturing arcticles, including containers and packaging materials, from hydraulically settable and inorganically filled materials are disclosed. Suitable compositions are prepared by mixing together a hydraulically settable binder or…
Andersen Per Just
Insulation barriers having a hydraulically settable component are disclosed. Such insulation barriers include laminate insulation barriers that have a highly insulative layer and a structural layer which has a hydraulically settable matrix. The highly insulative layer may…
Containers incorporating a hydraulically settable structural matrix including a hydraulically settable binder such as cement for use in the storing, dispensing, and/or packaging of food and beverage products are disclosed. The disposable and nondisposable food and beverage…
A method of manufacturing a cementitious composite includes: (1) forming mixing an extrudable cementitious composition by first forming a fibrous mixture comprising fibers, water and a rheology modifying agent and then adding hydraulic cement; (2) extruding the extrudable…
Apparatus and systems for finishing molded articles, such as fragile starch-bound articles, having flashing or other extraneous mold material attached thereto. The containers are conveyed from the mold apparatus to the flash removal system, which preferably includes a first…
A method of manufacturing a cementitious composite including: (1) mixing an extrudable cementitious composition by first forming a fibrous mixture comprising fibers, water and a rheology modifying agent and then adding hydraulic cement; (2) extruding the extrudable cementitious…
Design optimization methods can be used to design concrete mixtures having optimized properties, including desired strength and slump at minimal cost. The design optimization methods use a computer-implemented process that is able to design and virtually 'test' millions…
A method of manufacturing a cementitious composite including: (1) mixing an extrudable cementitious composition by first forming a fibrous mixture comprising fibers, water and a rheology modifying agent and then adding hydraulic cement; (2) extruding the extrudable cementitious…
A cementitious composite product that can function as a substitute for stone and solid surface materials, such as granite, marble, and engineered stone is provided. Furthermore methods for manufacturing the cementitious composite product using an extrudable cementitious…
A cementitious composite product that can function as a substitute for stone and solid surface materials, such as granite, marble, and engineered stone is provided. Furthermore methods for manufacturing the cementitious composite product using an extrudable cementitious…
A concrete composition having a 28-day design compressive strength of 3000 psi and a slump of about 5 inches is optimized to have high workability and a high strength to cement ratio. The concrete composition contains about 340 pounds per cubic yard hydraulic cement (e.g.…
Concrete compositions have a fine-to-coarse aggregate ratio optimized for increased workability with minimal segregation and bleeding. The concrete compositions include at least water, cement, coarse aggregate, and fine aggregate and have a slump of at least 1 inch and a 28-day…
A concrete composition having a 28-day design compressive strength of 4000 psi and a slump of about 5 inches is optimized to have high workability and a high strength to cement ratio. The concrete composition contains about 366 pounds per cubic yard hydraulic cement (e.g.,…
A cementitious composite product that can function as a substitute for stone and solid surface materials, such as granite, marble, and engineered stone is provided. Furthermore methods for manufacturing the cementitious composite product using an extrudable cementitious…
Concrete compositions have a fine-to-coarse aggregate ratio optimized for decreased viscosity and increased workability. The concrete compositions include at least water, cement, coarse aggregate, and fine aggregate and have a slump of at least 1 inch and a 28-day compressive…
A concrete composition having a 28-day design compressive strength of 4000 psi and a slump of about 5 inches is optimized to have high workability and a high strength to cement ratio. The concrete composition contains about 375 pounds per cubic yard hydraulic cement (e.g.,…
A cementitious composite product that can function as a substitute for stone and solid surface materials, such as granite, marble, and engineered stone is provided. Furthermore methods for manufacturing the cementitious composite product using an extrudable cementitious…
Design optimization methods can be used to design concrete mixtures having optimized properties, including desired strength and slump at minimal cost. The design optimization methods use a computer-implemented process that is able to design and virtually 'test' millions…
A method of manufacturing a cementitious composite includes: (1) forming mixing an extrudable cementitious composition by first forming a fibrous mixture comprising fibers, water and a rheology modifying agent and then adding hydraulic cement; (2) extruding the extrudable…
A molded cementitious architectural product for use in building construction has a cementitious body made of a molded cementitious material, the surface of which is polished (i e, burnished) to better resemble natural stone. The polished surface is formed by exposing a portion…
Concrete compositions have a fine-to-coarse particulates ratio optimized for decreased viscosity and increased workability. The concrete compositions include at least water, cement, coarse aggregate, and fine aggregate and have a slump of at least 1 inch and a 28-day compressive…
A concrete composition having a 28-day design compressive strength of 3000 psi and a slump of about 5 inches is optimized to have high workability and a high strength to cement ratio. The concrete composition contains about 299 pounds per cubic yard hydraulic cement (e.g.,…
A concrete composition having a 28-day design compressive strength of 4000 psi and a slump of about 5 inches is optimized to have high workability and a high strength to cement ratio. The concrete composition contains about 366 pounds per cubic yard hydraulic cement ( e.g .,…