A metallic article is fabricated by providing a die and a piece of a bulk-solidifying amorphous metallic alloy having a glass transition temperature. The bulk-solidifying amorphous metallic alloy is heated to a forming temperature of from about 0.75 T g to about 1.2 T g and…
Amorphous Technologies Interna
Solid die-cast articles are prepared from a charge of a bulk-solidifying amorphous alloy. The charge is heated to an injection temperature and injected into a die-casting mold. The charge is cooled at a rate, about 500° C. per second or less, such that its amorphous structure is…
A casting charge of a bulk-solidifying amorphous alloy is cast into a mold from a temperature greater than its crystallized melting temperature, and permitted to solidify to form an article. The oxygen content of the casting charge is limited to an operable level, as excessively…
A torsionally reacting spring, such as a helical spring, a torsion bar, or a torsion tube, requires the ability to torsionally deform elastically during service and return to its original, undeformed shape. The torsionally reacting spring is made of a bulk-deforming amorphous…
The surface features of an article are replicated by preparing a master model having a preselected surface feature thereon which is to be replicated, and replicating the preselected surface feature of the master model. The replication is accomplished by providing a piece of a…
A nickel tungsten-containing coating is electrodeposited onto a substrate from an electrodeposition bath having in solution from about 0.034 to about 0.047 moles per liter of nickel, from about 0.15 to about 0.28 moles per liter of tungsten, from about 0.13 to about 0.43 moles…
A hard-facing material source is an article whose net composition is, in weight percent, from about 20 to about 35 percent chromium, from about 2 to about 5 percent boron, from about 1 to about 2.5 percent silicon, from 0 to about 0.5 percent carbon, from about 0.5 to about 2…
A reinforcement-containing metal-matrix composite material is formed by dispersing pieces of reinforcement material throughout a melt of a bulk-solidifying amorphous metal and solidifying the mixture at a sufficiently high rate that the solid metal matrix is amorphous.…
A hardfacing apparatus includes a deposition head including a heat source, a hardfacing material source, and a chill block having a chill block surface. The deposition head is positioned at a location so as to deposit a mass of the hardfacing material onto the workpiece surface.…
A nickel tungsten-containing coating (30) is electrodeposited onto a substrate (34) from an electrodeposition bath having in solution from about 0.034 to about 0.047 moles per liter of nickel, from about 0.15 to about 0.28 moles per liter of tungsten, from about 0.13 to about…
A golf club (20) is made of a club shaft (22) and a club head (24). Either the club shaft (22) or the club head (24) is made at least in part of a bulk-solidifying amorphous metal. A preferred bulk-solidifying amorphous metal has a composition, in atomic percent, of from about…
An article includes a substrate and a composite material bonded to the substrate. The composite material includes a matrix consisting of a metallic alloy having a solidus temperature of at least about 700° C. and a plurality of unstabilized zirconium oxide particles distributed…
A nickel tungsten-containing coating (30) is electrodeposited onto a substrate (34) from an electrodeposition bath having in solution from about 0.034 to about 0.047 moles per liter of nickel, from about 0.15 to about 0.28 moles per liter of tungsten, from about 0.13 to about…
A nickel tungsten-containing coating (30) is electrodeposited onto a substrate (34) from an electrodeposition bath having in solution from about 0.034 to about 0.047 moles per liter of nickel, from about 0.15 to about 0.28 moles per liter of tungsten, from about 0.13 to about…
An article includes a substrate and a composite material bonded to the substrate. The composite material includes a matrix consisting of a metallic alloy having a solidus temperature of at least about 700° C. and a plurality of unstabilized zirconium oxide particles distributed…
A nickel tungsten-containing coating (30) is electrodeposited onto a substrate (34) from an electrodeposition bath having in solution from about 0.034 to about 0.047 moles per liter of nickel from about 0.15 to about 0.28 moles per liter of tungsten, from about 0.13 to about…
A hard-facing material source is an article whose net composition is, in weight percent, from about 20 to about 35 percent chromium, from about 2 to about 5 percent boron, from about 1 to about 2.5 percent silicon, from 0 to about 0.5 percent carbon, from about 0.5 to about 2…
Solid die-cast articles are prepared from a charge of a bulk-solidifying amorphous alloy. The charge is heated to an injection temperature and injected into a die-casting mold (176). The charge is cooled at a rate, about 500~C per second or less, such that its amorphous…
An article (20) includes a substrate (28, 30) and a composite material (22) bonded to the substrate (28, 30). The composite material (22) includes a matrix (40) consisting of a metallic alloy having a solidus temperature of at least about 700 °C and a plurality of unstabilized…
An article (20) includes a substrate (28, 30) and a composite material (22) bonded to the substrate (28, 30). The composite material (22) includes a matrix (40) consisting of a metallic alloy having a solidus temperature of at least about 700 °C and a plurality of unstabilized…
A golf club (20) is made of a club shaft (22) and a club head (24). Either the club shaft (22) or the club head (24) is made at least in part of a bulk-solidifying amorphous metal. A preferred bulk-solidifying amorphous metal has a composition, in atomic percent, of from about…