Sintered polybenzimidazole articles are obtained by compacting a particulate, dried polybenzimidazole resin under a pressure of 2,000 to 10,000 psi in a mold, heating the formed article to a temperature in the range of 825° to 950° F. for at least four hours, cooling the…
Assignee / Organization
Alpha Precision Plastics Inc
32Total Forward Citations
2Indexed Patents
16Avg Citations / Patent
1Portfolio H-Index
ABSTRACT OF THE DISCLOSURE Sintered polybenzimidazole articles are obtained by compacting a particulate, dried polybenzimidazole resin under a pressure of 2,000 to 10,000 psi in a mold, heating the formed article to a temperature in the range of 825 to 950°F for at least four…