Process for producing metal oxide powders by means of flame spray pyrolysis, in which an aerosol comprising a metal compound is introduced into a flame in a reactor and reacted therein, and the metal oxide powder obtained is separated from gaseous substances, wherein a) the…
Alff Harald
A copper oxide/silicon dioxide composite in spherical and/or spheroid form with an average particle diameter of 10 to 500 nm, containing 5 to 90% by weight silicon dioxide and 10 to 95% by weight copper oxide, wherein the composite particles are core-shell particles with…
Core-shell particles containing crystalline iron oxide in the core and amorphous silicon dioxide in the shell and in which a) the shell contains from 5 to 40% by weight of silicon dioxide, b) the core contains b1) from 60 to 95% by weight of iron oxide and b2) from 0.5 to 5% by…
Aluminium oxide powder in the form of aggregates of primary- particles, which has a BET surface area of from 10 to 90 m2/g and comprises as crystalline phases, in addition to gamma- aluminium oxide and/or theta-aluminium oxide, at least 30 % of delta-aluminium oxide. It is…
Aluminum oxide powder in the form of aggregates of primary-particles, which has a BET surface area of from 10 to 90 m2/g and comprises as crystalline phases, in addition to gamma-aluminum oxide and/or theta-aluminum oxide, at least 30% of delta-aluminum oxide. It is prepared by…
A process for producing a metal oxide powder proceeds by spray pyrolysis, in which a mixture comprising ammonia and an aerosol which is obtained by atomizing a solution containing a metal compound by means of an atomization gas is introduced into a high-temperature zone of a…
The invention relates to a method for producing a powdery mixed oxide A of the general formula Li 1+x (Ni a Co b Mn c )B d O 2 , where 0 < x ≤ 0.5; 0 < a ≤ 1; 0 ≤ b ≤ 1; 0 < c ≤ 1; 0.001 ≤ d ≤ 0.1, having a BET surface area of 10 to 50 m 2 /g and a tamped density of 250…
Process for the production of doped metal oxide particles, wherein the doping component is present on the surface in the form of domains, wherein in a first reaction zone, an oxidizable and/or -hydrolysable metal compound as dopant together with an atomization gas is atomized…
Core-shell particles which contain crystalline iron oxide in the core and amorphous silicon dioxide in the shell and in which a) the shell contains from 5 to 40% by weight of silicon dioxide, b) the core contains b1) from 60 to 95% by weight of iron oxide and b2) from 0.5 to 5%…
Core-shell particles containing crystalline iron oxide in the core and amorphous silicon dioxide in the shell and in which a) the shell contains from 5 to 40% by weight of silicon dioxide, b) the core contains b1) from 60 to 95% by weight of iron oxide and b2) from 0.5 to 5% by…
Process for the production of doped metal oxide particles, wherein the doping component is present on the surface in the form of domains, wherein in a first reaction zone, an oxidizable and/or - hydrolysable metal compound as dopant together with an atomization gas is atomised…
The invention relates to a method for producing a metal oxide powder by means of spray pyrolysis, in which a mixture containing ammonia and an aerosol, which is obtained by spraying a solution containing a metal compound by means of an atomizing gas, is introduced into a high…
Titanium-aluminium mixed oxide powder with a proportion of aluminium oxide of less than 1 wt.% or a proportion of titanium dioxide of less than 5 wt.%, wherein the sum of the proportions of titanium dioxide and aluminium oxide is at least 99.7 wt.%. It is produced by…