Patents
Assignee / Organization

Abe Fujio

46Total Forward Citations
13Indexed Patents
4Avg Citations / Patent
5Portfolio H-Index
JP 2005270958 A#5207059 Most Cited · 17 citations0.8/yr · PR 3.85ExpiredJP · Utility
Humidity conditioner and humidity conditioning method using the same
Inventors: Abe Fujio, Fujii Shigenobu, Ota TetsuoAssignee: Abe FujioFiled 2004-12-13

<P>PROBLEM TO BE SOLVED: To provide a humidity conditioner which is comparatively inexpensive but can condition humidity satisfactorily on the basis of excellent water absorbing/desorbing functions and can be used repeatedly and to provide a humidity conditioning method…

US 2007119301 A1#17771089 Most Cited · 6 citations0.3/yr · PR 1.61PendingUS · Application
Humidity conditioner and humidity conditioning method using the same
Inventors: Abe FujioAssignee: Abe FujioFiled 2005-02-25

The present invention is a humidity conditioner having a configuration in which one or more water-soluble polymers are introduced into a three-dimensional framework that is formed by one or more crosslinked water-absorbing polymers. Here, for the water-absorbing polymers, either…

US 2008216927 A1#16372942 Most Cited · 6 citations0.3/yr · PR 3.05PendingUS · Application
High Temperature Bolt Material

A high temperature bolt material, characterized in that it is a ferrite steel comprising 8 wt % or more of Cr and having a tempered martensite structure and can be used in a high temperature region of higher than 500° C.; and a method for producing the high temperature bolt…

WO 2004/087979 A1#16658181 Most Cited · 6 citations0.3/yr · PR 2.23PendingWO · Application
Welded joint of tempered martensite based heat-resistant steel

A welded joint of a tempered martensite based heat-resistant steel, characterized in that the fine grain portion in the weld heat-affected zone of a heat-resistant steel having a tempered martensite structure exhibits a creep strength of 90 % or more of the creep strength of the…

US 2006054253 A1#21492870 Most Cited · 5 citations0.2/yr · PR 1.38PendingUS · Application
Ferritic heat-resistant steel and method for producing it

The invention provides a ferritic heat-resistant steel having excellent high-temperature oxidation resistance, especially excellent steam oxidation-resistant characteristics. In high-Cr ferritic heat-resistant steel, ultra-fine oxide particles having a size of not larger than 1…

WO 02,061,162 A1#30587475 Most Cited · 3 citations0.1/yr · PR 1.21PendingWO · Application
Heat-resistant martensite alloy excellent in high-temperature creep rapture strength and ductility and process for producing the same

A heat-resistant martensite alloy in which (A) the composition consists of 0.03 to 0.15 wt.% carbon, 0.01 to 0.9 wt.% silicon, 0.01 to 1.5 wt.% manganese, 8.0 to 13.0 wt.% chromium, 0.0005 to 0.015 wt.% aluminum, up to 2.0 wt.% molybdenum, up to 4.0 wt.% tungsten, 0.05 to 0.5…

WO 2005/021806 A1#39366121 Most Cited · 2 citations0.1/yr · PR 1.03PendingWO · Application
High temperature bolt material

A high temperature bolt material, characterized in that it is a ferrite steel comprising 8 wt % or more of Cr and having a tempered martensite structure and can be used in a high temperature region of higher than 500°C; and a method for producing the high temperature bolt…

WO 2005/082525 A1#46885498 Most Cited · 1 citations0.1/yr · PR 1.04PendingWO · Application
Humidity conditioner and humidity conditioning method using the same
Inventors: Abe FujioAssignee: Abe FujioFiled 2005-02-25

The present invention is a humidity conditioner having a configuration in which one or more water-soluble polymers are introduced into a three-dimensional framework that is formed by one or more crosslinked water-absorbing polymers. Here, for the water-absorbing polymers, either…

TW 200,538,287 A#68587311 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredTW · Utility
Humidity conditioner and humidity conditioning method using the same
Inventors: Abe FujioAssignee: Abe FujioFiled 2005-02-25

The present invention is a humidity conditioner having a configuration in which one or more water-soluble polymers are introduced into a three-dimensional framework that is formed by one or more crosslinked water-absorbing polymers. Here, for the water-absorbing polymers, either…

WO 02,086,176 A1#71869553 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Ferritic heat-resistant steel and method for production thereof

A ferritic heat-resistant steel which comprises, in wt %, 1.0 to 13 % of chromium, 0.1 to 8.0 % of cobalt, 0.01 to 0.20 % of nitrogen, 3.0 % or less of nickel, 0.01 to 0.50 % of one or more elements selected from the group consisting of vanadium, niobium, tantalum, titanium,…

WO 02,086,176 A8#99733486 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Ferritic heat-resistant steel and method for production thereof

A ferritic heat-resistant steel which comprises, in wt %, 1.0 to 13 % of chromium, 0.1 to 8.0 % of cobalt, 0.01 to 0.20 % of nitrogen, 3.0 % or less of nickel, 0.01 to 0.50 % of one or more elements selected from the group consisting of vanadium, niobium, tantalum, titanium,…

WO 2005/082525 B1#110101227 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Humidity conditioner and humidity conditioning method using the same
Inventors: Abe FujioAssignee: Abe FujioFiled 2005-02-25

The present invention is a humidity conditioner having a configuration in which one or more water-soluble polymers are introduced into a three-dimensional framework that is formed by one or more crosslinked water-absorbing polymers. Here, for the water-absorbing polymers, either…