Patents
WO 2008/009801 A2#12838061 Most CitedPendingWIPO (PCT International)Application

Method for preparing a synthetic talc composition from a kerolite composition

8Forward Citations (#12838061 Global)
0.4/yrCitation Velocity (#18211741 Global)
2.28Citation PageRank (#11750205 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The invention relates to a method for preparing a synthetic talc composition. According to said method, a kerolite composition is subjected to an anhydrous thermal treatment carried out at a pressure lower than 5 bar, from over a few hours up to over a few days, at a treatment temperature higher than 300°C. The invention also relates to a synthetic talc composition prepared in this way, the synthetic talc particules of the composition being exclusively of chemical formula - (Si4)Mg3O10(OH)2 - and identifiable, during X-ray diffraction, by the presence of a characteristic diffraction peak located at a distance of between 9.40-9.68 Å and corresponding to a plane (001). Said synthetic talc particles also have a thermally stable crystalline structure of stacked laminae, which is very similar to that of a natural talc and has a particle size smaller than approximately ten micrometres.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 8.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.