Abstract
A process is described for producing an aluminum alloy sheet having excellent bendability for use in forming panels for automobiles. An aluminum alloy containing 0.50 to 0.75 by weight Mg, 0.7 to 0.85% by weight Si, 0.1 to 0.3% by weight Fe, 0.15 to 0.35% by weight Mn, and the balance Al and incidental impurities, is used and is semi-continuously cast into ingot. The cast alloy ingot is subjected to hot rolling and cold rolling, followed by solution heat treatment of the formed sheet. The heat treated sheet is quenched to a temperature of about 60 - 120°C and the sheet is then coiled. This coil is then pre-aged by slowly cooling the coil from an initial temperature of about 60 - 120°C to room temperature at a cooling rate of less than 10°C/hr. Another aluminum alloy containing 0.0 0.4 % by weightCu, 0.3 0.6 by weight Mg, 0.45 0.7 % by weight Si, 0.0 0.6 % by weight Mn, 0.0 0.4 % by weight Fe, up to 0.06 % by weight Ti, and the balance A1 and incidental impurities, is used and is semi-continuously cast into ingot. The cast alloy ingot is subjected to hot rolling and cold rolling, followed by solution heat treatment of the formed sheet. The heat treated sheet is quenched to a tempera
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 26.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 26 total)
References Cited — Backward Prior Art (10)
Non-Patent Literature (1)
- PATENT ABSTRACTS OF JAPAN vol. 2000, no. 05 14 September 2000 (2000-09-14)