Interconnector line of thin film, sputter target for forming the wiring film and electronic component using the same
Abstract
An interconnector line of thin film comprising 0.001 to 30 at % of at least one kind of a first element capable of constituting an intermetallic compound of aluminum and/or having a higher standard electrode potential than aluminum, for example, at least one kind of the first element selected from Y, Sc, La, Ce, Nd, Sm, Gd, Tb, Dy, Er, Th, Sr, Ti, Zr, V, Nb, Ta, Cr, Mo, W, Mn, Tc, Re, Fe, Co, Ni, Pd, Ir, Pt, Cu, Ag, Au, Cd, Si, Pb and B; and one kind of a second element selected from C, O, N and H in a proportion of 0.01 at ppm to 50 at % of the first element, with the balance comprising substantially Al. In addition to having low resistance, such an Al interconnector line of thin film can prevent the occurrence of hillocks and the electrochemical reaction with an ITO electrode. The interconnector line of thin film can be obtained by sputtering in a dust-free manner by using a sputter target having a similar composition.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 2.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A sputter target, consisting essentially of 0.001 to 30 at % of at least one first element constituting an intermetallic compound of Al, 0.01 at ppm to 50 at %, with respect to the amount of the first element, of at least one second element selected from the group consisting of C, O, N and H, provided that an amount of N is not more than 3000 at ppm, and the balance of Al.
- Claim 2Independent Claim
A sputter target, consisting essentially of 0.001 to 30 at % of at least one first element having a standard electrode potential higher than Al, 0.01 at ppm to 50 at %, with respect to the amount of the first element, of at least one second element selected from the group consisting of C, O, N and H, provided that an amount of N is not more than 3000 at ppm, and the balance of Al.
- Claim 3Depends on #2
The sputter target according to claim 2 , wherein the sp
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (32)
Non-Patent Literature (3)
- European Search Report dated Aug. 16, 1999.
- Office Action issued by the Japanese Patent Office on May 8, 2012, in Japanese Patent Application No. 2009-069802.
- Official Action issued by the Japanese Patent Office on Jan. 20, 2009, for Japanese Patent Application No. 2005-276819, and English-language Summary thereof.