Process for making high denier filaments of thermotropic liquid crystalline polymers and compositions thereof

3Forward Citations (#31497895 Global)
0.1/yrCitation Velocity (#41386378 Global)
1.15Citation PageRank (#34278272 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention discloses and claims a novel process for the formation of high denier as-spun and heat-treated filaments of a thermotropic liquid crystalline polymer. Preferred embodiments include process for the formation of as-spun and heat treated monofilaments of a few wholly aromatic polyesters and polyesteramides. The process involves (a) heating of a thermotropic liquid crystalline polymer to above its melting transition temperature; (b) passing said molten polymer through an extrusion chamber equipped with an extrusion capillary of an aspect ratio of greater than about 1 and less than about 15 to form a filament; and (c) winding the filament at a draw-down ratio of at least about 4. The filaments so formed are of at least 50 denier per filament (dpf) and feature essentially uniform molecular orientation across the cross-section. In a final optional step, the filaments are heat treated in stages to form filaments exhibiting excellent tensile properties. Both as-spun and heat-treated filaments feature remarkably good tensile properties retaining at least 80 to 90 percent of the properties expected of conventional low denier (5 to 10 dpf) filaments.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for forming an as-spun filament of a thermotropic liquid crystalline polymer having the following properties: (i) denier of at least about 50 denier per filament; (ii) tenacity of at least about 8 grams per denier; (iii) modulus of at least about 450 grams per denier; and (iv) elongation of at least about 2 percent; said process comprising the steps of: (a) heating a thermotropic liquid crystalline polymer to a temperature of at least about 15° C. above its melting transition to form a fluid stream of said thermotropic polymer; (b) passing said stream through a heated extrusion chamb

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • J. Appl. Polym. Sci. 1995, vol. 55 (p. 1489-1493).
  • J. Rheology 1992, vol. 36 (p. 1057-178).