Abstract
(Heat) In the disclosed heat -treating method of hot-rolled steel plate containing less than 0.20% of C, 0.05 to 0.40% of Si, 0.10 to 5.0% of Mn and 1.50 to 10.0% of Ni ( 1.5% to 10.0% Ni and 0.1% to 5.0% Mn and further at least one element selected from the group consisting of Mo, Cu, Cr, Nb and V, at need and) with the balance being substantially Fe, (comprising subjecting one or more time repeatedly said) the hot-rolled steel plate (to heating) is heated to (and sequent quenching from) a temperature (within) between the (range between) Ac1 and Ac3 transformation points and then cooled, whereafter (, then subjecting) the steel plate is subjected to tempering treatment at a temperature below the Ac1 point but sufficiently high so as to cause precipitation or formation of fine austenite, thereby to improve (largely) toughness at low temperature and to obtain excellent workability.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 52.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A HEAT-TREATING METHOD FOR PRODUCING A STEEL HAVING AN EXCELLENT TOUGHNESS AT AN EXTREMELY LOW TEMPERATURE AND A HIGH STRENGTH AND GOOD WORKABILITY FROM A STEEL CONSISTING ESSENTIALLY OF LESS THAN 0.20 WT. % C (.), 0.05 TO 0.40 WT. % SI, 0.10 TO 5.0 WT. % MN, 1.50 TO 10.0 WT.% NI AS A BASIC ALLOYING COMPONENT, WITH THE BALANCE BEING FE AND THE USUAL IMPURITIES, COMPRISING SUBJECTING A HOT-ROLLED STEEL PLATE HAVING THE SAID COMPOSITION TO A HEAT-TREATMENT COMPRISING HEATING TO A TEMPERATURE BETWEEN AC1 TRANSFORMATION POINT AND THE AC3 TRANSFORMATION POINT AND A SUBSEQUENT COOLING FROM THE SAID
- Claim 2Depends on #1
A method according to claim 1, wherein the heat-tre