Patents
US 9,986,644 B2#99464367 Most CitedActiveUnited States (USPTO)Utility

Process for the production of entry sheet for drilling and entry sheet

0Forward Citations (#99464367 Global)
0.0/yrCitation Velocity (#99464367 Global)
0.56Citation PageRank (#99464367 Global)
12Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for the production of an entry sheet for drilling a printed wiring board material, which process comprises forming a multi-layered water-soluble resin composition layer on at least one surface of a metal foil, wherein an aqueous solution of a water-soluble resin composition is applied to the metal foil, dried and solidified to form one water-soluble resin composition layer, the application, drying and solidification of the aqueous solution of the water-soluble resin composition are repeated at least once to form at least one water-soluble resin composition layer on the above one water-soluble resin composition layer, the multi-layered water-soluble resin composition layer is composed of these water-soluble resin composition layers, the multi-layered water-soluble resin composition layer has a thickness of at least 50 μm and is almost free from air bubbles, and an entry sheet for drilling a printed wiring board material obtained by the above process.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An entry sheet for drilling a printed wiring board material, comprising a metal foil and a multi-layered water-soluble resin composition layer formed on at least one surface of the metal foil, wherein: the thickness of each water-soluble resin composition layer of the multi-layered water-soluble resin composition layer is in the range of 10 μm to 50 μm, the thickness of the multi-layered water-soluble resin composition layer is at least 50 μm and the number of air bubbles having a diameter of at least 30 μm each in the multi-layered water-soluble resin composition layer is 20 or less per an ar

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (5)

  • "Mechanism of Bubble Formation During the Drying of Polymer Films" Reza Pourdarvish Mohammadi; the Pennsylvania State University (May 2005).
  • Chinese Office Action (with English translation) dated Jul. 11, 2011 in corresponding Chinese Application No. 200810187336.8.
  • Chinese Office Action dated Mar. 23, 2012 in corresponding Chinese Application No. 200810187336.8, with English translation thereof.
  • Indian Office Action dated Oct. 31, 2017 in corresponding Indian Patent Application No. 1303/DEL/2009.
  • Japanese Office Action dated Apr. 17, 2012 in corresponding Japanese Application No. 2008-330447, with English translation thereof.