Method for making low bend loss optical fiber preforms
Abstract
A method of making an optical fiber preform comprising in order: (i) manufacturing a glass preform with at least one porous layer; (ii) exposing the glass preform with at least one porous layer to a fluorine precursor at temperature below 1295° C. to make a fluorine treated preform, and (iii) exposing the fluorine treated glass preform with at least one porous silica based layer the temperatures above 1400° C. to completely sinter the preform. Preferably, the porous silica based layer of the glass preform exposed to fluorine precursor has average density of at least 0.7 g/cm 3 but less than 1.9 g/cm 3 .
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of making an optical fiber preform, the method comprising: manufacturing a glass preform with at least one porous layer; pre-densifying the glass preform comprising increasing an average density of the at least one porous layer such that the at least one porous layer has an average density of at least 0.7 g/cm 3 but less than 1.9 g/cm 3 , thereby forming a pre-densified preform; exposing the pre-densified preform to a fluorine precursor in a furnace having a doping temperature of 1290° C. or less to make a pre-densified fluorine doped preform; and exposing the pre-densified fluorine
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (30)
Non-Patent Literature (1)
- Tandon; "Doping of Silica During Sintering"; Journal of Non-Crystalline Solids; 351 (2005) 1466-1472.