Ion assisted deposition top coat of rare-earth oxide
Abstract
A method of manufacturing an article comprises providing an article. An ion assisted deposition (IAD) process is performed to deposit a second protective layer over a first protective layer. The second protective layer is a plasma resistant rare earth oxide having a thickness of less than 50 microns and a porosity of less than 1%. The second protective layer seals a plurality of cracks and pores of the first protective layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method comprising: performing an ion assisted deposition (IAD) process at a first deposition rate of 0.25-1.0 Angstroms per second to deposit a bottom portion of a second protective layer on at least a region of a first protective layer that is on a surface of an article, wherein the first deposition rate achieves improved conformance and better adherence of the second protective layer to the first protective layer than a higher deposition rate; and continuing the IAD process at a second deposition rate of 2-10 Angstroms per second to deposit a top portion of the second protective layer on t
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗