Patents
US 9,970,080 B2#50985031 Most CitedActiveUnited States (USPTO)Utility

Micro-alloying to mitigate the slight discoloration resulting from entrained metal in anodized aluminum surface finishes

1Forward Citations (#50985031 Global)
0.1/yrCitation Velocity (#42034267 Global)
0.85Citation PageRank (#50985031 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Micro additions of certain elements such as zirconium or titanium are added to high strength aluminum alloys to counter discoloring effects of other micro-alloying elements when the high strength alloys are anodized. The other micro-alloying elements are added to increase the adhesion of an anodic film to the aluminum alloy substrate. However, these micro-alloying elements can also cause slight discoloration, such as a yellowing, of the anodic film. Such micro-alloying elements that can cause discoloration can include copper, manganese, iron and silver. The micro additions of additional elements, such as one or more of zirconium, tantalum, molybdenum, hafnium, tungsten, vanadium, niobium and tantalum, can dilute the discoloration of the micro-alloying elements. The resulting anodic films are substantially colorless.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An enclosure for an electronic device, the enclosure comprising: an aluminum alloy substrate having (i) a non-discoloring element, and (ii) a micro-alloying element that is included in a concentration of a non-zero amount no greater than 0.10 weight %, or a concentration of about 0.10 weight %, of the aluminum alloy substrate; and an anodic film formed on the aluminum alloy substrate, wherein the micro-alloying element is incorporated within the anodic film and associated with discoloration of the anodic film, and the non-discoloring element is incorporated within the anodic film, thereby decr

  2. Claim 2Depends on #1

    The enclosure of claim 1 , wherein the micro-alloying element includes at least one of copper, manganese, iron or silver. 3

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 2,692,851 AMethod of forming hard, abrasionresistant coatings on aluminum and aluminum alloys195430
US 3,388,050 AAnodized aluminum alloy product196813
US 3,411,994 AAluminum anodizing process and product thereof196816
US 3,985,629 AMethod for color-anodizing aluminum and aluminum alloys in a short period of time197613
US 4,039,355 AAluminum alloy shapes197723
US 4,066,516 AMethod for forming colorless or colored pattern having shade difference on an aluminum or aluminum alloy article197840
US 4,483,751 AProcess of treating a nodic oxide film, printed wiring board and process of making the same198432
US 4,518,468 AProcess for making electrostatic imaging surface198536
US 4,606,796 AColored, anodized aluminum-base article and method of preparing same198656
US 4,631,112 ASurface-treated aluminum alloy substrates for magnetic disks198615
US 4,856,326 AApparatus for measuring an adhesion force of a thin film198961
US 4,894,127 AMethod for anodizing aluminum199063
US 4,987,766 AMethod for determining the micro impact energy capacity of the surface of a disk drive head and a thin film disk199117
JP H0347937 AAluminum alloy material having white color tone after subjected to anodic oxidation treatment—16
US 5,066,368 AProcess for producing black integrally colored anodized aluminum components199160
US 5,078,845 AProcess for preparing an electrode foil for use in aluminum electrolytic capacitors199235
US 5,277,788 ATwice-anodized aluminum article having an organo-phosphorus monolayer and process for making the article199487
US 5,336,341 AInfrared radiation element and process of producing the same199429
US 5,472,788 AColored anodized aluminum and electrolytic method for the manufacture of same199553
US 5,705,225 AMethod of filling pores in anodized aluminum parts199833
US 5,919,561 AReflector with resistant surface199953
US 6,027,629 AVacuum chamber made of aluminum or its alloys, and surface treatment and material for the vacuum chamber200083
EP 0,997,545 A1Ornamental aluminum alloy member and process for producing the same—7
CN 1,254,028 ADecorative aluminium alloy member and its production method—16
JP 2000313996 AAluminum composite member—27
CH 691,064 A5Reflector with high total reflection, resistant to mechanical stress and chemical corrosion—19
US 6,235,409 B1Aluminum laminate200149
US 6,339,958 B1Adhesion strength testing using a depth-sensing indentation technique200266
US 6,581,446 B1Determination of adhesion strength of HVOF coating by spherical indentation200320

Non-Patent Literature (5)

  • Achbach et.al. WADC technical report 55-150, Part VI, Project No. 7360, 1957.
  • Alwitt, R.S. and R.C. McClung , "Mechanical Properties of Anodized Aluminum Coatings"; Proceedings of the SUR/FIN7 '92, American Electroplaters and Surface Finishers Society, Atlanta, Georgia, Jun. 1992.
  • Brock, et al., "European Coatings Handbook", 2000, Curt R. Vincentz, (pp. 374-376), 5 Pages.
  • Charles Grubbs, "Anodizing of Aluminium", Metalfinishing, pp. 397-412, (16 Pages).
  • Chinese Application for Invention No. 201610011395.4-First Office Action dated Jul. 21, 2017.