Patents
US 9,963,756 B2#33865003 Most CitedActiveUnited States (USPTO)Utility

Method for production of martensitic steel having a very high yield point and sheet or part thus obtained

3Forward Citations (#33865003 Global)
0.4/yrCitation Velocity (#21614906 Global)
0.99Citation PageRank (#42187255 Global)
24Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a method for the fabrication of a martensitic steel sheet with a yield stress greater than 1300 MPa. The method includes the steps of obtaining a semi-finished steel product, the composition of which includes, whereby the contents are expressed in percent by weight: 0.15%≤C≤0.40%, 1.5%≤Mn≤3%, 0.005%≤Si≤2%, 0.005%≤Al≤0.1%, S≤0.05%, P≤0.1%, 0.025%≤Nb≤0.1%, and optionally: 0.01%≤Ti≤0.1%, 0%≤Cr≤4%, 0%≤Mo≤2%, 0.0005%≤B≤0.005%, 0.0005%≤Ca≤0.005%. The remainder of the composition is iron and the inevitable impurities resulting from processing. The semi-finished product is reheated to a temperature T 1 in the range between 1050° C. and 1250° C., then the reheated semi-finished product is subjected to a roughing rolling at a temperature T 2 in the range between 1050 and 1150° C., with a cumulative rate of reduction ϵ a greater than 100%, to obtain a sheet with a not totally recrystallized austenitic structure with an average grain size less than 40 micrometers and preferably less than 5 micrometers. The sheet is then cooled to prevent a transformation of the austenite at a rate V R1 greater than 2° C./s to a temperature T 3 in the range between 970° C. and Ar3

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    5%≤Mn≤3%, 0.005%≤Si≤2%, 0.005%≤Al≤0.1%, S≤0.05%, P≤0.1%; and 0.025%≤Nb≤0.1%, the remainder of the composition comprising iron and the inevitable impurities resulting from processing; heating the semi-finished product to a temperature T 1 between 1050° C. and 1250° C.; rolling the reheated semi-finished product in a roughing mill at a temperature T 2 between 1050 and 1150° C. with a cumulative reduction rate ϵ a greater than 100% to obtain a sheet with an austenitic structure, not fully recrystallized, with an average grain size

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 4,619,714 AControlled rolling process for dual phase steels and application to rod, wire, sheet and other shapes198646
JP S63134628 AProduction of hot rolled thick steel plate having high strength and high toughness—6
JP H01275719 AManufacture of thick steel plate having high strength and high toughness—6
CN 1,106,070 ALow-temp. weldable thin-grain steel plate—11
WO 9,932,672 A1Ultra-high strength steels with excellent cryogenic temperature toughness—10
CN 1,282,381 AUltra-high strength steels with excellent cryogenic temp. toughness—12
US 6,264,760 B1Ultra-high strength, weldable steels with excellent ultra-low temperature toughness200162
JP 2004010971 AMethod for producing steel sheet having excellent strength and toughness and satisfactory flatness at high efficiency—11
US 2008017283 A1Steel For Machine Structural Use With Excellent Strength, Ductility, And Toughness And Method For Producing The Same—8
JP 2008208454 AHigh-strength steel excellent in delayed fracture resistance and its production method—27
JP 2009215576 AMethod for producing rolled non-heat treated steel material—6
CN 101,586,217 ALow-cost and ultra-high strength and toughness martensite steel and manufacturing method thereof—15
CN 101,676,425 AMartensite abrasion-resistant steel with high strength and production produce thereof—21
JP 2010106287 AHigh-tension steel excellent in fatigue characteristic, and producing method thereof—16
WO 2010/055609 A1Thick steel sheet having high strength and method for producing same—11
JP 2010132945 AHigh-strength thick steel plate having excellent delayed fracture resistance and weldability, and method for producing the same—18
JP 2010159466 AHigh-tensile-strength steel material superior in fatigue characteristics and method for manufacturing the same—24
US 2010230016 A1High-strength steel plate and producing method therefor—11
JP 2010229512 AMethod for producing ferrite-pearlite type rolled non-heat treated steel material—4
EP 2,290,116 A1Thick steel sheet having high strength and method for producing same—9
JP 2011052321 AHigh-strength hot-rolled steel sheet having excellent low temperature toughness and method for producing the same—96
US 2011253271 A1High-strength steel plate and producing method therefor—16
US 2011259481 A1High Strength Steel Plate for Nuclear Reactor Containment Vessel and Method of Manufacturing the Same—13
US 2013095347 A1Hot-stamped steel, method of producing of steel sheet for hot stamping, and method of producing hot-stamped steel—46