Abstract
A method for providing a foamed, opacifying element includes providing a foamable aqueous composition, aerating it to a foam density of 0.1-0.5 g/cm 3 , applying the foamed aqueous composition to a porous substrate, drying, and densifying the dried layer. Such foamable aqueous compositions have 0.05-15 weight % of porous particles; at least 20 weight % of a binder; at least 0.0001 weight % of additives (including a surfactant); water; and at least 0.001 weight % of an opacifying colorant. Each porous particle includes a continuous polymeric phase and discrete pores; a mode particle size of 2-50 μm; and a porosity of 20-70 volume %. The continuous polymeric phase T g is >80° C. and has a polymer viscosity of 80-500 centipoises at an ethyl acetate shear rate of 100 sec −1 at a concentration of 20 weight % at 25° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 35 · Forward citations: 22.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for providing a foamed, opacifying element, the method comprising: providing a foamable aqueous composition that has at least 35% solids and up to and including 70% solids, and comprises: (a) at least 0.05 weight % and up to and including 15 weight % of porous particles, each porous particle comprising a continuous polymeric phase and a first set of discrete pores dispersed within the continuous polymeric phase, the porous particles having a mode particle size of at least 2 μm and up to and including 50 μm and a porosity of at least 20 volume % and up to and including 70 volume %, and
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗