US 9,945,480 B2#33860085 Most CitedActiveUnited States (USPTO)Utility

Piston assembly including a polymer coating with hard particles applied to sliding surfaces

3Forward Citations (#33860085 Global)
0.4/yrCitation Velocity (#21614535 Global)
0.99Citation PageRank (#42147412 Global)
39Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A piston assembly comprises a piston body, a connecting rod, and a wrist pin. The piston body includes a pair of first cross bores presenting a piston sliding surface. The connecting rod includes a second cross bore presenting a rod sliding surface which is axially aligned with the first cross bores of the piston body. A wrist pin is disposed in the aligned cross bores and couples the piston body to the connecting rod. The wrist pin also presents a pin sliding surface facing the rod sliding surface and the piston sliding surfaces. A coating is applied to at least one of the sliding surfaces, such as by dipping, brushing, atomizing, spraying, printing, or screen printing. The coating includes a polymer matrix, such as polyamide imide (PAI), and hard particles, such as Fe 2 O 3 , disposed throughout the polymer matrix. The hard particles have a hardness of at least 600 HV/0.5.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 39 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A piston assembly, comprising: a piston body including at least one first cross bore presenting a piston sliding surface; a wrist pin disposed in said at least one first cross bore, said wrist pin presenting a pin sliding surface facing said piston sliding surface; and a coating disposed on at least one of said sliding surfaces, said coating including a polymer matrix with hard particles disposed in said matrix, and said hard particles including Fe 2 O 3 .

  2. Claim 2Depends on #1

    The piston assembly of claim 1 , wherein said hard particles of said coating have a hardness of at least 600 HV/0.5 at a temperature of 25° C.

  3. Claim 3Depends on #1

    The piston assembly of claim 1 , wherein said hard particles of said coating have a D 50 particle size by volume not greater than 10.0 microns.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (39)

PatentTitleYearCitations
EP 0,024,291 A2Composite material for objects or layers with glossy or rough surfaces highly resistant to wear—14
US 4,440,069 AComposite piston and process198445
US 4,868,067 ACooperating slidable aluminum alloy members198922
US 4,898,905 ASliding material199056
JP H0422611 AManufacture of polymer composite molded object—4
US 5,239,955 ALow friction reciprocating piston assembly199356
US 5,257,603 ACoated piston and process for applying coating199345
JP H0624263 U内燃機関用ピストン構造—5
US 5,626,907 AProcess for coating metal surfaces with a fluororesin using a primer199761
US 5,670,010 AProcess for adhering a fluororesin film to a metal surface using a primer199732
US 5,677,372 ADiamond reinforced composite material199734
US 5,884,600 AAluminum bore engine having wear and scuff-resistant aluminum piston199959
EP 0,938,970 A2Bearing material with a plastic gliding layer—11
US 6,162,767 AComposite bearing with iron oxide additive200014
US 6,312,484 B1Nonwoven abrasive articles and method of preparing same200172
US 6,376,061 B1Composite multilayer material20028
JP 2002242933 ASlide bearing and manufacturing method thereof—15
US 2002155304 A1Sliding bearing and method of manufacturing the same—25
US 6,548,453 B1Continuously coated multi-composition, multi-layered solid lubricant coatings based on polyimide polymer compositions200321
US 6,557,457 B1Bushingless piston and connecting rod assembly and method of manufacture200347
US 6,770,381 B2Sliding bearing for internal combustion engine200421
WO 2004/070238 A2Wrist pin—5
JP 2005201289 AComposite for dry lubrication coat film formation—20
US 7,024,981 B2Wrist pin20067
DE 102005009552 A1Gegenstand mit reibungsvermindernder Beschichtung und Verfahren zur Herstellung einer Beschichtung—33
US 7,156,014 B2Compressor200710
US 2007000468 A1Coated power cylinder components for diesel engines—20

Non-Patent Literature (4)

  • Diamond Composite Technology, Process Specifications, Apr. 25, 2003, UK Abrasives, p. 1.
  • Endura Coatings World Headquarters, Polymer Composite Diamond Coating Specifications, 2012, Endura, p. 1 (note website discusses patents for composite diamond coatings going back a long time).
  • International Search Report PCT/US2012/062032 dated Feb. 5, 2013.
  • Wikipedia, Polyimide, Jun. 11, 2010, Wikipedia, 1-3.