Patents
US 9,941,135 B2#55980513 Most CitedActiveUnited States (USPTO)Utility

Methods of forming a hard mask layer and of fabricating a semiconductor device using the same

1Forward Citations (#55980513 Global)
0.1/yrCitation Velocity (#42304171 Global)
0.80Citation PageRank (#55980513 Global)
35Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of forming a hard mask layer on a substrate includes forming an amorphous carbon layer using nitrous oxide (N 2 O). A source of carbon and the nitrous oxide (N 2 O) are introduced to the substrate under a plasma ambient of an inert gas. The amorphous carbon layer has a nitrogen content ranging from about 0.05 at % to about 30 at % and an oxygen content ranging from about 0.05 at % to about 10 at %. In forming a semiconductor device, the hard mask layer is patterned, and a target layer beneath the hard mask layer is etched using the patterned hard mask layer as an etch mask.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 35 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a hard mask layer, comprising: providing a substrate; and introducing a source of carbon and nitrous oxide (N 2 O) to the substrate under a plasma ambient of an inert gas to form an amorphous layer of carbon on the substrate, wherein the nitrous oxide (N 2 O) is provided at a flow rate ranging from 10 sccm to 1000 sccm, and the amorphous carbon layer has a nitrogen content ranging from 0.05 at % to 30 at % and an oxygen content ranging from 0.05 at % to 10 at %.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the nitrous oxide (N 2 O) is excited under the plasma ambient to decompose C—C bonds in the amorphous carbon layer.

  3. Claim 3Depends on #1

    The method of claim 1 , further comprising introducing nitrogen (N 2 ) to the substrate at the same time as the nitrous oxide (N 2 O), wherein a flow rate of the nitrogen

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (35)

PatentTitleYearCitations
US 2004000534 A1Hardmask of amorphous carbon-hydrogen (a-C:H) layers with tunable etch resistivity—87
US 2004119163 A1Method of making semiconductor devices using carbon nitride, a low-dielectric-constant hard mask and/or etch stop—30
US 6,835,663 B2Hardmask of amorphous carbon-hydrogen (a-C:H) layers with tunable etch resistivity200415
US 2005214694 A1Pattern formation method—37
US 2005287771 A1Liquid precursors for the CVD deposition of amorphous carbon films—52
US 2006078677 A1Method to improve transmittance of an encapsulating film—37
US 7,079,740 B2Use of amorphous carbon film as a hardmask in the fabrication of optical waveguides200626
US 2007200179 A1Strain enhanced CMOS architecture with amorphous carbon film and fabrication method of forming the same—86
JP 2007224383 AMethod for forming amorphous carbon film, method for producing semiconductor device using the same and computer readable storage medium—12
KR 100,765,806 B1Method of depositing amorphous carbon layer200710
US 7,407,893 B2Liquid precursors for the CVD deposition of amorphous carbon films200819
US 2008260968 A1Method of forming amorphous carbon layer using cross type hydrocarbon compound and method of forming low-k dielectric layer using the same—7
US 2008293248 A1Method of forming amorphous carbon film and method of manufacturing semiconductor device using the same—13
JP 2008291344 AMethod of forming amorphous carbon film and method of manufacturing semiconductor device using the same—9
US 2009035584 A1Methods for device fabrication using pitch reduction and associated structures—42
KR 20090057533 AMethod of forming hard mask for semiconductor device—1
US 7,679,133 B2Vertical-type non-volatile memory devices2010849
KR 20100112070 AMethod for forming an amorphous carbon layer and method for forming a pattern using the same—9
US 2011233648 A1Three-Dimensional Semiconductor Memory Devices And Methods Of Fabricating The Same—903
US 8,222,162 B2Batch processing method for forming structure including amorphous carbon film20123
US 2012183887 A1Oriented amorphous carbon film and process for forming the same—9
JP 2012142574 AMethod of forming hard mask of metal oxide—19
US 2012258261 A1Increasing etch selectivity of carbon films with lower absorption co-efficient and stress—18
US 8,465,903 B2Radiation patternable CVD film20139
US 8,553,466 B2Non-volatile memory device, erasing method thereof, and memory system including the same2013790
US 8,559,235 B2Nonvolatile memory device, operating method thereof and memory system including the same2013808
KR 101,326,704 B1Batch processing method for forming structure including amorphous carbon film20132
KR 20140009169 AAtomic layer deposition of photoresist materials and hard mask precursors—7
US 8,654,587 B2Nonvolatile memory devices, channel boosting methods thereof, programming methods thereof, and memory systems including the same2014794

Non-Patent Literature (2)

  • Seok-Jun Won et al., “The Formation of an Almost Full Atomic Monolayer via Surface Modification by N2O-Plasma in Atomic Layer Deposition of ZrO2 Thin Films”, Chemistry of Materials Article(2009), 21, pp. 4374-4379.