Patents
US 9,932,657 B2#91287606 Most CitedActiveUnited States (USPTO)Utility

Method of making a Ni—based single crystal superalloy and turbine blade incorporating same

0Forward Citations (#91287606 Global)
0.0/yrCitation Velocity (#91287606 Global)
0.56Citation PageRank (#91287606 Global)
28Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a Ni-based single crystal superalloy which has the following composition by weight: 0.1 wt % or more and 9.9 wt % or less of Co, 5.1 wt % or more and 10.0 wt % or less of Cr, 1.0 wt % or more and 4.0 wt % or less of Mo, 8.1 wt % or more and 11.0 wt % or less of W, 4.0 wt % or more and 9.0 wt % or less of Ta, 5.2 wt % or more and 7.0 wt % or less of Al, 0.1 wt % or more and 2.0 wt % or less of Ti, 0.05 wt % or more and 0.3 wt % or less of Hf, 1.0 wt % or less of Nb and less than 3.0 wt % of Re with the remainder including Ni and unavoidable impurities. This Ni-based single crystal superalloy has a low Re content and also has excellent high-temperature strength, mainly creep strength.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a Ni-based single crystal superalloy which has the following composition by weight: 8.0 wt % of Co, 7.0 wt % of Cr, 1.8 wt % of Mo, 8.2 wt % of W, 6.0 wt % of Ta, 5.2 wt % of Al, 1.6 wt % of Ti, 0.10 wt % of Hf, and 0.8 wt % of Re with the remainder including Ni and unavoidable impurities, and wherein said superalloy contains no Nb or contains it as an unavoidable impurity, wherein the Ni-based single crystal superalloy is obtained by performing a solution heat treatment and an aging treatment to an alloy ingot which has the above-described composition, and wherein th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (28)

PatentTitleYearCitations
JP S53146223 ANickellbased superalloy product and method of making some—6
GB 1,592,237 AHeat treated superalloy single crystal article and process—4
JP S5919032 ALeveling of distortion of steel plate—10
US 4,582,548 ASingle crystal (single grain) alloy198647
US 4,643,782 ASingle crystal alloy technology1987128
US 4,719,080 AAdvanced high strength single crystal superalloy compositions1988209
GB 2,234,521 ANickel-base superalloys for producing single crystal articles having improved tolerance to low angle grain boundaries—37
CA 2,048,756 A1Single crystal, environmentally-resistant gas turbine shroud—1
US 5,100,484 AHeat treatment for nickel-base superalloys199279
US 5,154,884 ASingle crystal nickel-base superalloy article and method for making199272
RU 2,026,399 C1Monocrystal heat-resistant nickel alloy with low density19952
JP H0770679 AHigh corrosion resistant and high strength cemented carbide, high corrosion resistant and high strength single crystal casting, gas turbine and combined cycle generating system—6
US 5,489,194 AGas turbine, gas turbine blade used therefor and manufacturing method for gas turbine blade199642
JP H11246924 ANi-base single crystal superalloy, its production, and gas turbine parts—9
US 6,054,096 AStable heat treatable nickel superalloy single crystal articles and compositions200036
US 6,159,314 ANickel-base single-crystal superalloys, method for manufacturing the same, and gas turbine parts prepared therefrom200015
EP 1,184,473 A2Nickel-base single-crystal superalloys, method of manufacturing same and gas turbine high temperature parts made thereof—25
US 2003041930 A1Modified advanced high strength single crystal superalloy composition—60
EP 1,431,405 A1Nickel base superalloy—15
US 2004221925 A1Ni-based superalloy having high oxidation resistance and gas turbine part—47
WO 2006/067189 A1A ni based alloy, a component, a gas turbine arrangement and use of pd in connection with such an alloy—20
WO 2007/037277 A1Nickel-base superalloy with excellent unsusceptibility to oxidation—8
RU 2,297,466 C2Monocrystal nickel heat-resistant alloy200711
WO 2007/122931 A1Ni-BASE SUPERALLOY AND METHOD FOR PRODUCING SAME—4
EP 1,876,263 A1Heat-resistant member—7
US 2008112814 A1Method for the heat treatment of nickel-based superalloys—2
US 2011076180 A1Nickel-Based Superalloys and Articles—13
US 8,771,440 B2Ni-based single crystal superalloy20146

Non-Patent Literature (5)

  • Canadian Office Action dated Nov. 22, 2012 issued in corresponding Canadian Patent Application No. 2,764,664.
  • Chinese Office Action and English translation dated Mar. 6, 2013 issued in corresponding Chinese Patent Application No. 201080028753.3.
  • Extended European Search Report and European Search Opinion dated Feb. 4, 2015 in corresponding European Patent Application No. 10808201.7 (10 pages).
  • International Search Report and Written Opinion dated Nov. 2, 2010 in corresponding PCT International Application No. PCT/JP2010/063486.
  • N. Saunders et al., "Modelling the Material Properties and Behaviour of Ni-Based Superalloys," Superalloys 2004 (TMS, 2004), pp. 849-858.