Patents
US 9,932,429 B2#4049605 Most CitedActiveUnited States (USPTO)Utility

Method for producing porous articles from alternating poly(ethylene tetrafluoroethylene) and articles produced therefrom

21Forward Citations (#4049605 Global)
2.6/yrCitation Velocity (#1192482 Global)
1.96Citation PageRank (#15021681 Global)
19Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Poly(ethylene tetrafluoroethylene) (ETFE) polymers having an average molecular weight of at least 300,000 g/mol and a melt enthalpy of at least 57 J/g are provided. The ETFE polymer may include at least one additional comonomer. The ETFE polymer is used to form a porous tape or membrane that has a node and fibril structure. A porous ETFE tape may be formed by lubricating the ETFE polymer and subjecting the lubricated polymer to pressure at a temperature below the melting point of the ETFE polymer. Optionally, the ETFE tape may be expanded at a temperature below the melting temperature of the ETFE polymer to form an expanded ETFE membrane. Alternatively, the ETFE polymer may subjected to heat and pressure without the addition of a lubricant to form a dense preform. The dense preform may be subsequently slit in a length direction and stretched to form a dense ETFE fiber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 21.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A microporous poly(ethylene tetrafluoroethylene) (ETFE) article comprising: a microporous ETFE tape formed from an ETFE polymer having an average molecular weight of at least about 300,000 g/mol, a melting point from about 260° C. to 300° C., and a melt enthalpy of at least 57 J/g, said tape having a node and fibril structure.

  2. Claim 2Depends on #1

    The microporous article of claim 1 , wherein, said ETFE polymer includes from about 0.001 mol % to about 10 mol % of an additional monomer.

  3. Claim 3Depends on #1

    The microporous article of claim 1 , wherein said ETFE tape has a thickness from about 0.01 to about 4 mm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Arai et al., Influence of alternating sequential fraction on the melting and glass transition temperatures of ethylene-tetrafluoroethylene copolymer, Elsecier Ltd, Polymer 51, pp. 4831-4835, 2010.
  • Tuminello et al., Rheological Molecular Weight Distribution Determinations of Ethylene/Tetrafluoroethylene Copolymers: Implications for Long-Chain Branching, American Chemical Society, Macromolecules 26, 499-503, 1993.