Strengthening glass containers
Abstract
A glass container and related methods of manufacturing a glass container. A solution having a composition including a silane, a solvent, a catalyst, and water, is applied to an exterior glass surface of the glass container, at an application temperature between 5 and 40 degrees Celsius, such that the solution at least partially fills the surface imperfections to provide a room-temperature-curable cold-end coating on the glass container. Then, the applied solution is allowed to cure on the exterior glass surface of the glass container, at a curing temperature between 5 and 40 degrees Celsius.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of filling surface imperfections in an exterior glass surface of a glass container that includes the steps of: (a) applying a solution including an amphiphile, a solvent, a catalyst, and water to the exterior glass surface of the glass container, at an application temperature between 5 and 40 degrees Celsius, such that the solution at least partially fills the surface imperfections to provide a room-temperature-curable cold-end coating on the glass container; (b) directly and within 60 seconds after completing step (a), rinsing the glass container with a liquid, including water, at a
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.