Method for producing porous articles from ultra high molecular weight polyethylene

40Forward Citations (#1422208 Global)
5.0/yrCitation Velocity (#280400 Global)
3.38Citation PageRank (#6238658 Global)
18Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Ultra high molecular weight polyethylene (UHMWPE) polymers that have an average molecular weight of at least 500,000 g/mol and an enthalpy of at least 190 J/g is provided. The UHMWPE polymer may include at least one comonomer. The UHMWPE polymer is used to form a membrane, that, when expanded, has a node and fibril structure. The UHMWPE membrane has an endotherm of about 150° C. associated with the fibrils in the membrane. The membrane has a percent porosity of at least 25%, and in exemplary embodiments, the percent porosity is at least 60%. Additionally, the UHMWPE membrane has a thickness less than 1 mm. An UHMWPE membrane may be formed by lubricating the UHMWPE polymer, subjecting the lubricated polymer to pressure at a temperature below the melting point of the UHMWPE polymer to form a tape, and expanding the tape at a temperature below the melting temperature of the UHMWPE polymer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 40.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for making a porous ultra high molecular weight polyethylene (UHMWPE) membrane comprising: lubricating an ultra high molecular weight polyethylene polymer having a molecular weight of at least about 500,000 g/mol and only a single endotherm with a melt enthalpy of at least about 190 J/g to form a lubricated polymer; subjecting said lubricated polymer to pressure at a temperature below a first melt temperature of said ultra high molecular weight polyethylene polymer to form a tape; and expanding said tape at a temperature below the first melt temperature of said ultra high molecular w

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • A. P. Pickles, R.S. Webber, K.L. Alderson, P. J. Neale, "The effect of the processing parameters on the fabrication of auxetic polyethylene Part 1 the effect of compaction condiitons" Journal of Materials Science 30 (1995) pp. 4059-4068.
  • International Search Report dated May 26, 2014 for PCT/US2014/013945.
  • K. L. Alderson, A. P. Kettle, P. J. Neale, A. P. Pickles, "The effect of the processing parameters on the fabrication of auxetic polyethylene. Part II the Effect of sintering temperature and time", Journal of Material Science 30, (1995), pp. 4069-4075.
  • K.L. Alderson, R. S. Webber, and K, E. Evans, "Microstructural evolution in the processing of auxetic microporous polymers" Physica Status Solidi (b) 244, No. 3, (2007), p. 828-841.
  • P. J. Neale, A. P. Pickles, K. L. Alderson, "The effect of the processing parameters on the fabrication of auxetic polyethylene, Part III the effect of extrusion conditions", Journal of Material Science 30, (1995), pp. 4087-4094.